Casting factors in horizontal intermittent continuous casting of commercial pure aluminum such as drawing speed and draw-and-stop cycle were examined. A prolonged cycle of draw-and-stop is required with increases in pitch-length and drawing speed. The casting rate is accelerated with an increase in pitch-length up to 40mm and keeps constant at pitch-length above 40mm. Solidification proceeds both in stopping and drawing periods. Coarse columnar grains in the strip cast at 10mm of a pitch incline toward the reverse direction of casting. The strip cast at 80mm of a pitch has coarse columnar grains which incline toward the reverse direction of casting and needle-like columnar grains periodically.
- 一般社団法人 軽金属学会の論文
一般社団法人 軽金属学会 | 論文
- Mechanical and wear properties of SiC whisker/ADC12 aluminum alloy composites fabricated by die casting.
- Joining of aluminum and ceramics.
- タイトル無し
- Undercooling and solidification behavior of fluid clumps of second-poured melt of hypereutectic Al-Si alloy in Duplex Casting process.
- Change in apparent viscosity of stirred slurry during production of semi-solid hypereutectic Al-Si alloy by slurry-melt mixing process.