5083および7075合金のストレッチ・ゾ-ン解析による破壊じん性評価
スポンサーリンク
概要
- 論文の詳細を見る
An attempt to evaluate the fracture toughness of 5083 and 7075 alloys is made by observing the stretched zone (SZ) formed ahead of pre-crack in a Charpy test. The width and height of the stretched zone (SZW and SZH) analyzed stereographically from fracture toughness. Twice SZH corresponds to the critical crack tip opening displacement (CTODc). The plane strain fracture sunface. (K1c) estimated from CTODc measured is in good agreement with the valid K1c already informed. The fracture toughness is sufficiently appreciable by measuring SZ even in small size test pieces. A proportional relation is found between SZW and SZH. Plastic blunting of crack tip advances up to 60 to 70° in a particular direction.
- 一般社団法人 軽金属学会の論文
一般社団法人 軽金属学会 | 論文
- Mechanical and wear properties of SiC whisker/ADC12 aluminum alloy composites fabricated by die casting.
- Joining of aluminum and ceramics.
- タイトル無し
- Undercooling and solidification behavior of fluid clumps of second-poured melt of hypereutectic Al-Si alloy in Duplex Casting process.
- Change in apparent viscosity of stirred slurry during production of semi-solid hypereutectic Al-Si alloy by slurry-melt mixing process.