Pitting corrosion of aluminum in synthetic supply water
スポンサーリンク
概要
- 論文の詳細を見る
A pitting corrosion characteristic of pure aluminum in supply water, artificially synthetized from Ca2+, Mg2+, HCO-3, Cl-, SO42-, SiO32- and free chrorine, was studied. Experimental results showed that free chlorine, SiO32- and Ca2+ were harmful in producing pitting of aluminum in water. However, effects of HCO3-, Mg2+ and Cl- on pitting were hardly recognized. Interaction among the above constituent species was almost absent in pitting corrosion of aluminum. The results of the present study were analyzed by applying the statistical theory of the extreme value, proposed by P. M. Aziz.
- 一般社団法人 軽金属学会の論文
一般社団法人 軽金属学会 | 論文
- Mechanical and wear properties of SiC whisker/ADC12 aluminum alloy composites fabricated by die casting.
- Joining of aluminum and ceramics.
- タイトル無し
- Undercooling and solidification behavior of fluid clumps of second-poured melt of hypereutectic Al-Si alloy in Duplex Casting process.
- Change in apparent viscosity of stirred slurry during production of semi-solid hypereutectic Al-Si alloy by slurry-melt mixing process.