BWRオリフィス下流配管における減肉位置予測解析
スポンサーリンク
概要
- 論文の詳細を見る
To increase load factor of nuclear power plants, it is necessary to decrease the number of days needed for periodic inspection and the number of days of unplanned outages. One of the countermeasures for these issues is to establish a prediction method for pipe wall thinning. There are two phenomena to be considered in pipe wall thinning. They are flow accelerated corrosion (FAC) and liquid droplet impingement erosion (LDI). In boiling water reactors (BWRs), LDI tends to influence pipe wall thinning more than FAC does. LDI is the wall thinning phenomena caused by droplet impingement. It is necessary to develop an appropriate method to predict the location of wall thinning. In this paper we compared measured data with computational analysis results for the location of wall thinning. By defining that the droplet frequency distribution had double peaks at the extrapolated location from the wall of an orifice toward downstream, we were able to predict the central location of the large reduction in thickness with a difference of less than about 0.2D[mm](D: pipe diameter) from the measured location in the flow direction at the elbow.
著者
-
久恒 眞一
日立geニュークリア・エナジー(株)
-
椎名 孝次
(株)日立製作所 日立研究所
-
浜田 紀昭
(株)日立製作所 日立研究所
-
大塚 雅哉
(株)日立製作所 日立研究所
-
坪内 邦良
(株)日立製作所 電力・電機開発研究所
-
岩原 光太郎
日立GEニュークリア・エナジー(株)
-
久恒 眞一
日立GEニュークリア・エナジー(株)
関連論文
- 局所減肉を有するエルボ配管の低サイクル疲労挙動
- 局所減肉を有するエルボ配管の静的破損挙動評価
- 1250 局部減肉がエルボ配管の低サイクル破損挙動に及ぼす影響(G03-8 材料力学(8)疲労・強度1,21世紀地球環境革命の機械工学:人・マイクロナノ・エネルギー・環境)
- BWRオリフィス下流配管における減肉位置予測解析
- 内圧が作用するエルボ配管の低サイクル疲労挙動に及ぼす局部減肉の影響 : 修正共通勾配法に基づく疲労寿命評価