The optimization of additive contents and presintering conditions for Si-additive mixture granules
スポンサーリンク
概要
- 論文の詳細を見る
Determined by the strength, flowability, and microstructure of the granules, the optimization of additive contents and presintering conditions for Si-additive mixture granules was assessed. Excessive additive contents led to a low granular strength and poor flowability due to the formation of large agglomerates and voids. The optimum presintering temperature for a 3 wt % Y2O3–Al2O3–CaO system was found between 1300 and 1375°C. Temperatures below and above the optimum temperature range resulted in low strength and poor flowability, respectively. The packing configuration by porous granules was modeled to calculate the intergranular porosity and intragranular porosity out of the total porosity.
- 公益社団法人 日本セラミックス協会の論文
著者
-
SONG In-Hyuck
Engineering Ceramics Group, Korea Institute of Materials Science
-
PARK Young-Jo
Engineering Ceramics Research Group, Korea Institute of Materials Science
-
LEE Jae-Wook
Engineering Ceramics Research Group, Korea Institute of Materials Science
関連論文
- Effect of aluminum hydroxide content on porosity and strength of porous mullite-bonded silicon carbide ceramics
- The optimization of additive contents and presintering conditions for Si-additive mixture granules