A Method for Preparing New Elongated-Shaped Silica Sols.
スポンサーリンク
概要
- 論文の詳細を見る
An active silicic acid sol was added to a mixture of a Ca(NO<SUB>3</SUB>)<SUB>2</SUB> aqueous solution and a NaOH aqueous solution, then the mixture was heated for several hours under stirring at 100–150°C to obtain a silica sol. The silica sol consisted of elongated-shaped colloidal particles desirable for film formation.
- 公益社団法人 日本化学会の論文
著者
-
Tanimoto Kenji
Central Research Institute, Nissan Chemical Industries, Ltd.
-
Yoshida Akitoshi
Central Research Institute, Nissan Chemical Industries, Ltd.
-
Watanabe Yoshitane
Central Research Institute, Nissan Chemical Industries, Ltd.
-
Andoo Mikio
Central Research Institute, Nissan Chemical Industries, Ltd.