TiB<SUB>2</SUB>-5%TaB<SUB>2</SUB>-CoB and TiB<SUB>2</SUB>-5%W<SUB>2</SUB>B<SUB>5</SUB>-1%CoB materials have higher transverse rupture strength, hardness and density than those of TiB<SUB>2</SUB>-1%CoB materials. The strengthening mechanism of both types materials, TiB<SUB>2</SUB>-5%TaB<SUB>2</SUB>-1%CoB and TiB<SUB>2</SUB>-5%W<SUB>2</SUB>B<SUB>5</SUB>-1%CoB, has been discussed. The higher transverse rupture strength of the both materials has been caused mainly by suppressing grain growth of TiB<SUB>2</SUB> with the solid solution between TiB<SUB>2</SUB> and TaB<SUB>2</SUB>, or between TiB<SUB>2</SUB> and W<SUB>2</SUB>B<SUB>5</SUB>, and caused secondarily by the lattice strain of TiB<SUB>2</SUB>, and reduction of residual pores.
- 社団法人 粉体粉末冶金協会の論文
著者
関連論文
- ワイヤ切断法における作用砥粒に関する-考察
- Ge単結晶のワイヤ切断実験
- TiN-TiB2系のホットプレス焼結
- TiB2基焼結体に関する研究
- TiB2-5%TaB2-1%CoBおよびTiB2-5%W2B5-1%CoB焼結体の強化機構
- TiB2-TaB2基サーメットの機械的性質に及ぼす結合剤の影響
- TiB2基サーメットの機械的性質に及ぼす結合剤および二ホウ化金属添加の影響