Investigating that how the fatigue strength of high manganese cast steel is influenced by grain size, decarburization and embrittlement of carbide precipitation and also the effect of shotpeening there obtained the underwritten results.(1) The grain size dependancy of fatigue limit is relatively small comparing with that of structural steels, and the coarser it becomes the lower the fatigue limit with the rate of 0.5kg/mm2/grain size number.(2) The reduction in the fatigue strength due to decarburization is smaller than that of structural steels. This is because that the micro structure of outer layer changes into hard martensite from austenite due to decarburization.(3) The temper brittleness makes the fatigue limit raised as hardening follows after precipitation.(4) The shotpeening is effective for improving the fatigue strength of various surface finish and it makes the fatigue limit raised up from 6 to 25%.
- 大同特殊鋼株式会社の論文
著者
関連論文
- 耐熱鋳鋼HHの熱疲労特性について(高温強度小特集)
- 1-20 軸受鋼の転動疲れ寿命に及ぼす酸素および硫黄の影響
- 148 棒鋼の矯正太りの機構について(集合組織・介在物・その他, 加工・製鋼, 日本鉄鋼協会第 75 回(春季)講演大会講演)
- 1-9 耐熱鋳鋼 HH の熱疲労特性について
- 軸受鋼の機械的諸特性に及ぼす酸素,硫黄の影響
- 熱処理用トレー材SCH13の熱疲労強度
- 棒鋼の矯正太り
- 遅れ破壊強度に及ぼす冷間および温間転造の効果
- 摩擦接合用高力ボルトの遅れ破壊強度に及ぼす形状の影響
- 高Mn鋳鋼の疲労強度
- 小型片持ち式疲労試験機とこれによる2, 3の実験結果
- P.I 溶解材の特質について