Dephosphorization Treatment of High Phosphorus Iron Ore by Pre-reduction, Air Jet Milling and Screening Methods
スポンサーリンク
概要
- 論文の詳細を見る
This paper proposes a novel process for the pre-treatment of high phosphorus iron ore by pre-reduction, air jet milling and screening methods. The dephosphorization behavior was evaluated as a function of such parameters as the milling gas kinetic energy, Ek and specific energy consumption, Esp. At a fixed milling gas kinetic energy, the dephosphorization treatment behavior was highly dependent on the solids feed rate and the degree of sintering of the pre-reduced phases. The proposed pre-treatment process involves a pre-reduction process by carbonaceous materials at 1200°C, and air jet milling using Ek of 325.24 kJ and Esp of 3.24 kJkg–1h followed by fine screen separation using a 25 μm screen size.
論文 | ランダム
- RC-FDTD法におけるMatched DNGスラブからの不要な反射波軽減のための新しい境界条件
- DNGスラブ上水平ダイポールアンテナのモーメント法解析
- - EBG構造太陽電池モジュールによる電磁波反射抑制
- B-1-150 反射板付き線状アンテナアレーの受信電力と再放射電力(B-1.アンテナ・伝播B(アンテナ一般),一般講演)
- ダイズの木部溢泌液の窒素化合物組成に対する化合窒素の影響