Recycling Process for Sinter-Active U3O8 Powders
スポンサーリンク
概要
- 論文の詳細を見る
The effect of the oxidation temperature of UO2 pellets on the powder properties of oxidized U3O8 powders has been investigated. The powder morphology, crystalline size, and BET surface area of recycled U3O8 could be modified by controlling the oxidation temperature of the UO2 pellets. Recycled U3O8 powder with a high BET surface area and a small particle size could be obtained by lowering the oxidation temperature. It was also found that this low-temperature-oxidized sinter-active U3O8 powder is effective in mitigating the density drop of the UO2 pellets when the recycled U3O8 powder is added. Moreover, the recycled powder acted as a grain-size-enlarging promoter in the UO2 pellets.
著者
-
RHEE Young
Innovative Nuclear Fuel Division, Korea Atomic Energy Research Institute
-
YANG Jae
Innovative Nuclear Fuel Division, Korea Atomic Energy Research Institute
-
KIM Keon
Innovative Nuclear Fuel Division, Korea Atomic Energy Research Institute
-
KANG Ki
Innovative Nuclear Fuel Division, Korea Atomic Energy Research Institute
-
SONG Kun
Innovative Nuclear Fuel Division, Korea Atomic Energy Research Institute
関連論文
- Recycling Process for Sinter-Active U3O8 Powders
- Fabrication of Sintered Annular Fuel Pellet for HANARO Irradiation Test
- Recycling Process for Sinter-Active U_3O_8 Powders