The Studies on Micro-Structural Defects in Deformed Composite Matrix of Al-Si-Mg and SiC
スポンサーリンク
概要
- 論文の詳細を見る
Detailed Fourier line shape analysis has been performed on three different compositions of the composite matrix of Al-Si-Mg and SiC. The alloy composition in wt% is Al-7%Si, 0.35%Mg, 0.14%Fe and traces of copper and titanium (〜0.01%) with SiC varying from 0 to 30wt% in three steps i.e., 0, 10 and 30wt%. The line shift analysis has been performed by considering 111, 200, 220, 311 and 222 reflections after estimating their relative shift. Peak asymmetry analysis has been performed considering neighbouring 111 and 200 reflections and Fourier line shape analysis has been performed after considering the multiple orders 111 and 222, 200 and 400 reflections. Combining all these three analyses it has been found that the deformation stacking faults both intrinsic α' and extrinsic α" are absent in this alloy system whereas the deformation twin β has been found to be positive and increases with the increase of SiC concentration. So, like other Al-base alloys this ternary alloy also shows high stacking fault energy, and the addition of SiC introduces deformation twin which increases with its concentration in the deformed lattices.
- 社団法人応用物理学会の論文
- 1999-11-15
著者
-
Karmakar G.
Regional Engineering College
-
SEN R.
Regional Engineering College
-
MEIKAP A.-K.
Regional Engineering College
-
CHATTOPADHYAY S.-K.
Regional Engineering College
-
CHATTERJEE S.-K.
Regional Engineering College
-
SURAPPA M.-K.
Department of Metallurgy Indian Institute of Science
-
Sen R
Regional Engineering College