The observation of enhanced T_c in calcium free Tl compounds Tl_2Ba_2Cu_1O_x (2201) with varying concentration of Tl and Cu has been reported. Three different starting compositions (2201, 1201 and 2202) were studied extensively with varying conditions of preparation. Under the optimised conditions: sintering temperature 970℃ and duration 3-10 minutes the highest T_c (onset) 〜115 K and T_c (zero) 〜95 K was found. The XRD studies showed the transformation of all the three nominal compositions into 2201 phase with different T_cs.
- 社団法人応用物理学会の論文
- 1990-04-20
著者
-
Sharma C.
National Physical Laboratory
-
Suri D.
National Physical Laboratory
-
Chandra Subhas
National Physical Laboratory
-
Asthana Pavas
National Physical Laboratory
-
SAINI K.
National Physical Laboratory
-
EKBOTE S.
National Physical Laboratory
-
AGNIHOTRY S.
National Physical Laboratory
関連論文
- Behaviour of Ionic Effects on Response Times of Surface Stabilized Ferroelectric Liquid Crystal Devices
- Dynamics of Helix Winding, Unwinding and Switching of Ferroelectric Liquid Crystals
- 1H1045 施肥土壌からのN_2OとNOの発生制御要因
- Anisotropic Surface Anchoring Conditions for Gray-Scale Capability in High-Tilt-Angle Ferroelectric Liquid Crystal
- Total-Reflection Switch Using High-Tilt-Angle Cholesteric : Smectic C^* Phase Transition Ferroelectric Liquid Crystal
- The Enhancement of T_c in Calcium Free Tl-Bilayer Superconducting System (Tl_2Ba_2Cu_1O_x)
- Frequency Dependent Polarization Reversal and the Response Time of Ferroelectric Liquid Crystal by Triangular Wave Method
- Removal of Zig-Zag Defects in Surface-Stabilized Ferroelectric Liquid Crystal Cells