以固態燒結法研製場放射顯示器之ZnGa_2O_4螢光粉
スポンサーリンク
概要
- 論文の詳細を見る
ZnGa_2O_4 phosphor obtained from the first fired process is low luminance intensity and low efficiency. By the treatment of secondary fired process, the maximum luminance intensity and efficiency of ZnGa_2O_4 phosphor obtained by the second fired treatment process are 2050 cd/m^2 and 0.198 lm/W, respectively. The CIE chromaticity coordinate of ZnGa_2O_4 phosphor is at X = 0.1696, Y = 0.1608. The emission color of ZnGa_2O_4 phosphor is blue.
- 1997-02-14
著者
-
Yang Su-Hua
Deprtment of Electrical Engineering, National Cheng Kung University
-
Yokoyama Meiso
Deprtment of Electrical Engineering, National Cheng Kung University
-
Yang S‐h
National Kaohsiung Univ. Applied Sci. Kaohsiung Twn
-
楊 素華
Deprtment Of Electrical Engineering National Cheng Kung University
-
横山 明聰
國立成功大學 電機工程研究所
-
横山 明聰
Department Of Electrical Engineering National Cheng Kung University
-
横山 明聰
Deprtment of Electrical Engineering, National Cheng Kung University
関連論文
- 以固態燒結法研製場放射顯示器之ZnGa_2O_4螢光粉
- 以固態燒結法研製場放射顯示器之ZnGa_2O_4螢光粉
- 以連續性真空蒸鍍系統研製對角線十英吋ZnS:Mn薄膜電激發光顯示屏
- High Efficiency ZnS:Mn Thin Film Electroluminescent Device Fabricated by MOCVD
- 以連續性真空蒸鍍系統研製對角線十英吋ZnS:Mn 薄膜電激發光顯示屏