2種類のnear-αチタン合金のフレッティング疲労特性
スポンサーリンク
概要
- 論文の詳細を見る
In order to investigate the basic fretting fatigue properties of two kinds of near-α titanium alloy, fretting fatigue tests were carried out under axial loading conditions using a bridge-type contact plece. The influence of contact pressure on fretting fatigue properties was also investigated. The main results obtained are as follows. In both materials, fretting reduced the fatigue lives by a factor of four as a result of the initiation of the fatigue crack at early stage of life and acceleration of the crack propagation rate. Fretting fatigue lives decreased with increasing contact pressure. The difference in fretting fatigue lives among the materials used is explained by different of tangential force coefficients and fatigue crack growth properties, as well as compressive residual stress introduced by shot peening.
- 一般社団法人日本機械学会の論文
- 1997-06-25
著者
関連論文
- 無冷却構造としたセラミックス基複合材料製燃焼器の燃焼性能特性
- 2748 BNコートHi-Nicalon繊維強化複合材料の熱サイクル疲労(S18-2 セラミックス(2),S18 セラミックスおよびセラミックス系複合材料)
- Hi-Nicalon繊維を用いたトランスピレーション冷却構造を有するセラミックス基複合材料の熱サイクル試験結果
- 冷却構造を有するセラミックス基複合材料の熱サイクル下の耐久性に与える加圧冷却空気及び繊維間隔の影響
- F-1507 3次元織りSiC_f/SiCの高温強度特性(S54-2 耐熱材料・耐熱構造(2))(S54 耐熱材料・耐熱構造)
- 金属基複合材料製ファン動翼の耐衝撃強度特性
- 三次元織物構造とした耐熱複合材料SiCf/SiCの高温強度特性
- 231 セラミックス基複合材料製ディスクの破壊機構(OS 先進材料の力学的特性と計測技術)
- セラミックス基複合材料製ディスクの常温回転試験
- セラミックス基複合材料製ディスクの破壊機構
- タービン動翼とディスク嵌合部のフレッティング疲労特性
- 三次元織りセラミック基複合材料の高温酸化特性
- 粉末Ni基超合金製ディスクの繰返し回転試験による疲労き裂進展挙動(ボルトホールき裂の場合)
- 粉末Ni基超合金製ディスクの繰返し回転試験による疲労き裂進展挙動(ディスクボアき裂の場合)
- 334 ジェットエンジン用回転部品のフレッティング疲労(OS フレッティング摩耗と疲労)
- 高温摺動ベアリングの基礎特性について
- 122 near-αチタン合金の低サイクルフレッティング疲労
- セラミック基複合材料の航空機用エンジン部品への適用研究
- 113 高温加熱保持を行った3次元織セラミックス基複合材料の非破壊評価(セラミックス,一般セッション)
- 先進耐熱複合材料SiCf/SiCの強度特性(第1報)高温酸化の影響
- B-13 次期固定翼哨戒機用エンジン(XF7-10)の部品構造強度試験の概要(構造,一般講演)
- 技術総説 航空エンジン用先進耐熱材料の研究動向
- 先進耐熱複合材料SiCf/SiCの強度特性(第2報:強化繊維および織物構造の影響)
- 第2回フレッティング疲労に関する国際会議に参加して
- 2種類のnear-αチタン合金のフレッティング疲労特性