Mixtures of Ca(OH)2, Al2O3 and ZnO corresponding to 100-80 (3CaO+Al2O3)+0-20 (ZnO) in composition were treated hydrothermally at temperatures between 120°C and 300°C in saturated steam condition. The treated specimens were examined with an X-ray diffractometer and a polarizing or electron microscope.The results obtained were as follows.1) The mixture of 3CaO+Al2O3 gave Ca3Al2(OH)12 at temperatures between 120°C and 220°C and a mixture of Ca3Al2(OH)12+Ca4Al6O10(OH)6+Ca(OH)2 at temperatures between 230°C and 300°C.2) The mixtures of 98-80 (3CaO+Al2O3)+2-20 (ZnO) gave mixtures of Ca3Al2(OH)12+ZnO at temperatures between 120°C and 170°C, Ca3Al2(OH)12+Ca(OH)2+ZnAl2O4 at temperatures between 180°C and 220°C and Ca3Al2(OH)12+Ca4Al6O10(OH)6+Ca(OH)2+ZnAl2O4 at temperatures between 230°C and 300°C.3) The crystals of Ca3Al2(OH)12 were appeared as characteristic dodecahedrons ranging from 4μm to 10μm in diameter. ZnAl2O4 were appeared as granular crystals ranging from 1μm to 5μm in diameter.
- 社団法人日本セラミックス協会の論文
- 1976-01-01
著者
関連論文
- ハイアルミナセメントの水和と導電性
- 高炉水砕スラグ-セッコウ-消石灰系セメントの蒸気およびオ-トクレ-ブ養生
- 高硫酸塩スラグセメントモルタルの炭酸化と消石灰懸濁溶液処理
- 高炉水砕スラグ-セッコウ-消石灰系セメント硬化体の強度および組成 (スラグ特集)
- 蒸気養生による緑泥石-絹雲母-石英-セッコウー石灰系多孔質材料の製造に関する基礎的研究
- 厚形スレ-ト製造へのオ-トクレ-ブ養生の適用とその利点
- 333 酸化亜鉛混和による海水成分含有セメントモルタル中の鉄板腐食防止(セメント・コンクリート)
- セメントによるクロームメッキ廃水スラッジの処理に関する研究
- 微粉砕フライアッシュの可能性 微粉砕フライアッシュにアルカリを添加し大量混和した速硬セメントモルタル・コンクリートの強度特性
- ZnO添加Ca_3Al_2O_6組成調合物の熱水処理による生成物
- 最近の本邦におけるセメント基礎研究の動向
- キャスタブルの自由水と導電性
- 電気抵抗法によるアルカリ骨材反応の早期評価
- 骨材のアルカリ骨材反応に対する抵抗性
- 320 セメントモルタル ライニング鉄板の腐食に及ぼす微量金属酸化物混和剤の影響(セメント・コンクリート(I))
- 319 海水構成成分と鉄筋の腐食に関する自然電位及び微構造(セメント・コンクリート(I))
- 334 高静水圧下で硬化したセメントペーストの特性(セメント・コンクリート・岩石)
- 高炉水砕スラグ-セッコウ系硬化体の微構造
- Ba_2SiO_4セメント硬化体の耐硫酸性
- [17] 海水による鋼材発錆に関する基礎研究 ; 自然電位と細孔(腐食・防食)
- 1133 反応性骨材を使用したモルタルの電気抵抗特性(アルカリ骨材反応)
- [30] 載荷履歴をもつモルタルの強度発現と微細構造(物性)
- [25] セメントモルタルの熱衝撃抵抗性と微細構造(物性・強度・試験I)