ガスケット係数について(第2報)
スポンサーリンク
概要
- 論文の詳細を見る
In the previous paper of the authors, experimental and analytical studies were made on the influencing factors in asbestos-joint sheet gasket affecting the tightening characteristics under the pressure of internal fluid up to 20 Kg/cm^2. In the present paper, the authors propose an empirical formula regarding the relation between the gasket factor and leak pressure. And the authors made further analytical discussions in the paper about the condition in which the internal diameter of gasket was of constant quantity in the influencing factors and the width and thickness were of variable quantity, and the internal fluids applied were water and machine oil. In the present paper, experimental and analytical studies were made under the condition in which all the width and the internal diameter are of variable quantitics and the internal pressure applied ranges between 1 to 60 Kg/cm^2. The specimens tested in our experiments are asbestos-joint sheet, synthetic rubber and vinyle chloride gaskets.
- 社団法人日本材料学会の論文
- 1964-04-15
著者
関連論文
- 高温における低炭素鋼の切欠きクリープ破断に関する一考察 : クリープ中における切欠き材および平滑材の応力分布の変化
- 構成水圧力下の多結晶金属材料のクリープ変形に関する研究
- 2-18 静水圧力下における塑性加工装置の試作と二, 三の実験結果について
- 2-17 高圧力下の塑性加工に関する研究 : 第 1 報 圧縮加工実験装置と二, 三の実験
- 単純圧縮パッキンに対する密封機構の一考察
- 209 簡易長周期高温低サイクル疲労試験機の試作と寿命評価に係わる二三の実験結果(高温低サイクル疲労・構成式)
- 232 クリープ域における高温低サイクル疲労の切欠き効果に関する研究 : 変位制御と荷重制御との違いおよびき裂発生に注目して
- 高温における1Cr-1 Mo-1/4V 鋼の切欠きクリープ破壊に関する研究
- 高温におけるlCr-1Mo-l/4V鋼の切欠きクリープ破壊 : とくに,破断寿命に及ぼす試験片断面形状および真空ふん囲気の影響について
- 3-23 高温における ∣Cr-&mdi;Mo-1/4V 鋼の切欠きクリープ破壊 : とくに断面形状および真空雰囲気の影響について
- 高静水圧および軸引張荷重を受ける金属材料のクリープ試験装置
- ガスケット係数について(第2報)
- ガスケット係数について(第1報)
- ねじの強度に関する実験的研究
- 高温下におけるガスケットの性能について
- ガスケット係数の経過時間依存性に関する研究
- 石綿ジョイントシートガスケット材の静的挙動について
- (ボルト締)フランジ継手におけるガスケットの性能について
- ねじの強度における実験的考察