CrまたはNiを添加した高マンガンオーステナイト鋼のころがり疲労強度
スポンサーリンク
概要
- 論文の詳細を見る
The rolling contact fatigue tests were carried out on high manganese austenitic steel to investigate the influence of Cr or Ni addition on the rolling contact fatigue strength by using a Nishihara-type wear testing machine under a lubricated state with a relative slip ratio of -9%. The results obtained are summarized as follows: (1) The rolling contact fatigue limit of high manganese austenitic steel containing Cr or Ni was lower than that of high manganese austenitic steel having the standard chemical composition. (2) The rolling contact fatigue limit of high manganese austenitic steel remarkably increased by the work hardening phenomenon which is generated by repeat contact stress. (3) A crack of high manganese austenitic steel propagated along the boundary of the work hardening zone and the unwork hardening zone in the parallel direction with the contact surface. Its depth was deeper than the region where the stress value calculated according to the maximum shearing stress theory reached the maximum.
- 社団法人日本材料学会の論文
- 1988-02-15
著者
関連論文
- 軟鋼のころがり疲労に及ぼすTiNコーティングの影響
- 軟鋼のころがり疲労に及ぼす溶体化処理直後からの負荷運転の影響
- 高クロム鋳鉄のころがり疲労強度特性
- 軟鋼のころがり疲労に及ぼす溶体化処理温度の影響
- 高マンガンオーステナイト鋳鋼のころがり疲労強度に及ぼす結晶粒径の影響
- CrまたはNiを添加した高マンガンオーステナイト鋼のころがり疲労強度
- オーステナイト系ステンレス鋼(SUS304)のころがり疲労強度に及ぼす加工硬化の影響について
- 合金白鋳鉄のころがり疲労強度に及ぼす共晶炭化物の影響について
- まだら鋳鉄のころがり疲労強度について
- 片状および球状黒鉛鋳鉄のころがり疲労強度に及ぼす黒鉛の影響について
- 白鋳鉄のころがり疲労強度について