ステレオマッチングによるストレッチ・ゾーンの解明
スポンサーリンク
概要
- 論文の詳細を見る
Stereo measurements of the stretched region in the fracture toughness specimens used for J-integral tests were carried out by examining the shape and the angle to the crack plane with a scanning electron microscope. It was found that the shape of the stretched zone consisted of two portions, one of which forms a gradual slope and the other a steep slope to the plane of pre-crack. The scatter of the measured values of the angle of the stretched zone to the crack plane was very large, ranging from 10 to 48 degrees. However, in many cases the angle was about 33 degrees. As the result of stereo matching observations, unsymmetrical profiles of the stretched zone were often found even though the widths were equal in a pair of the fracture surfaces. As compared with the scanning and transmission electoron fractographs taken from the same stretched zone, the same features in size were obtained from both fractographs.
- 1980-06-15
著者
関連論文
- Ti-6Al-4V合金の疲労強度に及ぼすショットピーニングの影響
- Ti-6Al-4V合金の疲労き裂伝ぱ挙動に及ぼす異方性の影響(フラクトグラフィ特集)
- アルミ合金および軟鋼のストライエーション間隔の統計的検討 : 定量的疲労破壊事故解析へのフラクトグラフィの適用
- 赤外線応力画像システムを用いた疲労き裂検出の試み
- 赤外線応力画像システムによる各種切欠き近傍の応力評価
- 溶接部材および接合材の破損解析
- 溶接継手の疲労き裂伝ぱのフラクトグラフィ
- STS42鋼溶接継手の疲労き裂伝ぱ挙動に及ぼす残留応力の影響(疲労特集)
- フラクトグラフィによる機械部門の疲労破損解析
- 4.疲労に及ぼす影響因子I : 材料, 切欠き, 残留応力等の影響 : 疲労-基礎と設計への展開
- 低温における疲労き裂伝ぱのフラクトグラフィ的検討
- p分布プログラム荷重下の疲労き裂進展の評価
- SUS304鋼およびA533B鋼の溶接継手における疲労き裂伝ぱ挙動
- フラクトグラフィによる破損した機械部品の稼動応力振幅の推定
- 軟鋼突合せ溶接継手の疲労き裂伝ぱ挙動に及ぼす試験片寸法および形状の影響
- 突合せ溶接材および母材の疲労き裂伝ぱ挙動
- 炭素鋼の疲労き裂伝ぱ挙動に及ぼす微視的組織の影響
- 高強度鋼の疲労き裂伝ぱ機構に及ぼす微視的組織の影響 : 疲労き裂伝ぱ速度と旧オーステナイト粒径との関連
- ステレオマッチングによるストレッチ・ゾーンの解明
- 共析鋼の疲労き裂伝ぱ機構に及ぼす微視的組織の影響
- マッチングによる疲労破面形態の解明
- 4.疲労に及ぼす影響因子I : 材料, 切欠き, 残留応力等の影響 : 疲労-基礎と設計への展開