配管用伸縮管継手二層ベローズの高温疲労強度
スポンサーリンク
概要
- 論文の詳細を見る
In order to investigate the fatigue stregth of bellows at elevated temperature, fatigue tests at room temperature and 500℃, and stress analyses have been conducted on the manufactured bellows. The manufactured bellows are a two-ply type, in which strain can be decreased by axial extension and compression without loss of stiffness against pressure. It was found that the strain distribution changed with the bellows thickness and usually the maximum strain appeared at the outer surface of the root in the outer bellows. In order to estimate the fatigue lifetime of bellows, the octahedral shearing strain derived from both the axial and circumferential strains was found to be more effective than the estimation with only the axial strain, which is commonly used. Fatigue cracks were produced in the maximum atrain area, and the cracks propagated from the outer surface to the inner surface of the bellows. It seems that the strain intensity factor obtained from the measured strain is effective for estimation of fatigue crack propagation rates.
- 社団法人日本材料学会の論文
- 1989-04-15
著者
-
安部 英昭
(株)日立製作所エネルギー研究所
-
安部 英昭
(株) 日立製作所エネルギー研究所
-
下屋敷 重広
(株) 日立製作所エネルギー研究所
-
前田 納
(株) 日立製作所日立工場
-
下屋敷 重広
日立 エネルギー研
関連論文
- 疲労き裂挙動特性に及ぼす高温ナトリウムの環境効果
- 201 ナトリウム中耐熱衝撃材料の試作と強度評価
- 液体金属ナトリウムによるサーマルストライピングの下のき裂進展停留挙動
- 237 316FR 鋼のナトリウム中疲労強度特性
- Na中サーマルストライピングによる浸炭材の停留き裂
- 配管用伸縮管継手二層ベローズの高温疲労強度
- TiN皮膜の高温ナトリウム中における腐食挙動
- クロムカーバイト基ガス溶射皮膜の液体Na中における自己融着機構
- クロムカーバイト基溶射皮膜の高温Na中における腐食挙動
- Corrosion behavior of chromium in sodium polysulphide.
- Decontamination test of Mn from stainless steel by chemical decontamination process.
- Thermoelectric Performance of Iron Disilicide Thin Film Prepared by Preferential Oxidation.