SCS-6/Ti-24Al-11Nb複合材の熱疲労破損における環境の重要性と界面せん断強度(<特集>複合材料)
スポンサーリンク
概要
- 論文の詳細を見る
Thermal fatigue tests of an unidirectional SiC fiber reinforced Ti-24Al-11Nb matrix composite, SCS-6/Ti-24Al-11Nb, have been carried out without external load in air and in vacuum, under various thermal cycle conditions. The fiber employed was a β-SiC fiber of 140μm diameter with a carbon rich graded silicon carbide coating on the surface : SCS-6. This paper covers the following characteristics of the material subjected to thermal fatigue, compared with those subjected to long term isothermal exposure : (i)change of the visible crack density with thermal cycling ; (ii)change of the fiber/matrix interface morphology by means of EPMA and SEM ; (iii)change of the interfacial shear strength by the push-out tests, and(iv)effect of environment on the properties from(i)to(iii). Based on these systematic investigations, special attentions are paid to understand the mechanisms and mechanics of thermal fatigue failure, and how thermal fatigue damage should be assessed.
- 社団法人日本材料学会の論文
- 1999-05-15
著者
関連論文
- 3.次世代ガスタービン用超合金とコーティング材の高温強度(「超」あるいは「極」の技術と高温強度)
- 611 SiC 連続繊維強化 Ti 合金基複合材 SCS-6/SP700 の熱機械的疲労強度
- Ni基ODS合金とNi基超合金の拡散接合と接合体の高温疲労強度(高温強度)
- SiC連続繊維強化Ti-24Al-11Nb基複合材料の安定き裂成長過程
- SCS-6/Ti-24Al-11Nb複合材の熱疲労破損における環境の重要性と界面せん断強度(複合材料)
- 225 SCS-6 連続繊維強化チタニウム基複合材の疲労強度に及ぼすマトリックス組織の影響
- SiC連続繊維強化Ti-24Al-11Nb基複合材料の熱疲労損傷機構
- SiC連続繊維強化Ti-24Al-11Nb基複合材料の熱疲労損傷発達
- 115 SCS-6/Ti-24Al-11Nb 複合材の界面強度評価と熱疲労損傷
- 102 SCS-6/Ti-24Al-11Nb 複合材の熱サイクル損傷と破壊抵抗変化
- 予損傷を受けた結晶制御Ni基超合金中に生成されるセル状変質域の悪影響度低減化の試み : 補修およびリコーティング技術のために
- 予損傷を受けた CMSX-4 中のセル状変質域による疲労寿命低下防止のための新規概念コーティング : 単結晶 Ni 基超合金の補修技術のために(高温強度)
- 610 単結晶 Ni 基超合金の損傷治癒コーティングの長時間相互拡散挙動
- 単結晶Ni基超合金の高温疲労強度低下抑制用溶射皮膜の開発
- 609 コーティングを援用した単結晶 Ni 基超合金中の稼働損傷の治癒とその長時間安定性
- 5.3.耐熱・耐環境コーティングの最近の動向(5.材料力学)(機械工学年鑑)
- 720 繰返し負荷を受ける TBC 材の自然発生型剥離き裂
- 予損傷を受けた単結晶Ni基超合金におけるセル状変質域生成と高温疲労強度への影響(高温強度)