PHOSPHATE RELEASE FROM SYNTHETIC GLASSES AND INHIBITION OF PHOSPHATE FIXATION ON FERRIC HYDROXIDE
スポンサーリンク
概要
- 論文の詳細を見る
Release of phosphate from glasses in the systems basalt-K_3PO_4,granite-K_3PO_4,K_2SiO_3Na_2SiO_3-apatite has been studied. Equilibrium leachate concentrations in water are attained in 3-5 hr(K^+, 5-60μg cm^<-3>; PO_4^<3->, 2-15μg cm^<-3>). Glass composition, pH, and grain size influence solubility.Phosphate fixation on freshly precipitated Fe(OH)_3 and on iron-rich laterites appear to be inhibited when glasses are rich in Na-K silicates. This may be due to surface modification of Fe(OH)_3 by the formation of sodium ferric silicates which are known to be stable at low temperatures.
- 社団法人日本土壌肥料学会の論文
著者
-
Fyfe William
Geology Department University Of Western Ontario
-
KRONBERG Barbara
Geology Department, University of Western Ontario
-
LEONARDOS Othon
Geoscience Department, University of Brasilia
-
Leonardos Othon
Geoscience Department University Of Brasilia
-
Kronberg Barbara
Geology Department University Of Western Ontario