0.85%C-3%Cr ロール鋼の破壊靱性に及ぼす熱処理の影響
スポンサーリンク
概要
- 論文の詳細を見る
Fracture process of band-type spalling which often occurs on the barrel surface of cold rolling work rolls, is known to be controlled by the fracture toughness K_<IC> of the roll steel in many cases. In order to study the factors improving the K_<IC> value, fracture toughness tests were carried out on the test pieces which were taken from the actual roll of 0.85%C-3%Cr steel, and were quenched and tempered in several conditions. The main results obtained are as follows : (1) K_<IC> values were highly dependent on the hardness. In the same hardness level, the higher the austenitizing temperature was, the higher the K_<IC> value became, and as for the subzero treatment, non-subzero steel gave higher K_<IC> values. (2) In comparison between fully quenched steel and slack quenched steel containing some lower bainite in its structure, the latter gave higher K_<IC> values.
- 社団法人日本鉄鋼協会の論文
- 1988-10-01
著者
関連論文
- 大型バックアップロールの軸キー溝の応力解析と形状の検討
- 中心孔を有する大型バックアップロールの破壊事故品の応力解析と材料強度評価による検討
- 0.85%C-3%Cr ロール鋼の破壊靱性に及ぼす熱処理の影響
- 光弾性法による閉式孔型ロールの応力解析と形状の検討
- 562 非鉄用熱間圧延ロール鋼のヒートチェックと焼もどし温度との関係(マルエージ鋼・ローター・ロール・工具鋼・レール・線材, 材料, 日本鉄鋼協会 第 105 回(春季)講演大会)
- 306 キャリバーロールの応力解析と形状の検討 : 光弾性によるロール内部の応力解析第 3 報(圧延ロール・軸受・討論会, 加工, 日本鉄鋼協会 第 99 回(春季)講演大会)
- 305 6 段ミル用ロールの応力解析 : 光弾性によるロール内部の応力解析第 2 報(圧延ロール・軸受・討論会, 加工, 日本鉄鋼協会 第 99 回(春季)講演大会)
- 304 中心孔を有するバックアップロールの応力解析 : 光弾性によるロール内部の応力解析第 1 報(圧延ロール・軸受・討論会, 加工, 日本鉄鋼協会 第 99 回(春季)講演大会)
- 535 破壊靭性のロール材への適用(ロール材・電磁鋼板, 性質, 日本鉄鋼協会 第 98 回(秋季)講演大会)
- アルミニウム連続鋳造用0.55%C-1.1%Cr-0.5%Moロ-ル鋼の耐熱き裂性に及ぼす熱処理の影響