Continuous experiment was performed on a industrial scale for the production of sponge iron by using tunnel kiln furnace. Crushed ores were classified into two parts of which one consists of the size 10∿40mm, and another of the size under 10mm. The latter were crushed again up to all under 30 mesh. Ores of the size 10∿40mm were mixed with fine coke and put in chamotte containers. Fine ore was mixed with suitable amount of carburising medium. The mixture was put in a chamotte container in such way as not to mix with the reducing coke. These containers were placed on a car, which ran through the kiln. The max. temp of the kiln was kept at about 1300℃. The seduced products were solid mass of sp. gr. about 3.5. The sp. gr. of 7 may be obtained, if desired, by suitably charging conditions. According to this experiment it was shown that the sponge iron might be easily produced by tunnel kiln.
- 社団法人日本鉄鋼協会の論文
- 1944-02-25
著者
関連論文
- トンネル窯による原鐵製造の工業試驗結果
- ガスに依る粒鐵の脱硫(第 1 報)
- 39 ロータリーキルンによる砂鉄粒鉱の製造(製銑および製鋼, 第 55 回講演大会講演大要)
- 17 砂鉄製酸化粒鉱および還元粒鉱の開放型電気炉による製錬試験(製銑・製鋼(造塊), 日本鉄鋼協会第 56 回(秋季)講演大会講演大要)
- 粒鐵製造中規模試驗
- 海綿鐵製造を目的とせる磁鐵鑛の還元 (II) : 大塊の還元
- 海綿鐵製造を目的とせる磁鐵鑛の還元 (I) : 小塊の還元と之に伴ふ體積, 比重及び氣孔率の變化
- 熱河産含チタン鐵鑛の製錬研究
- 弓長嶺粉鑛よりスクラップ代用品を製造する試驗
- 砂鐵製錬の研究
- 粒鐵 (Luppe) 製造の一方法
- 低級チタン酸化物の鑛滓に及ぼす影響