概要
- 論文の詳細を見る
The austenite recrystallization behaviors during the hot-deformation and the characteristics of the ferrite-pearlite structures transformed during continuous cooling from the hot-deformed austenite were investigated for the medium carbon steels containing 0.4% carbon with 0 to 0.3% vanadium. The results are as follows : (1) The vanadium additions inhibit the recrystallization of hot-deformed austenite and elevate the austenite recrystallization temperatures in the medium carbon steels, more effectively than those in the low carbon steels. The austenite recrystallization-stop temperature of 0.4% carbon steel added 0.3% vanadium is over 200K higher than that of 0.4% carbon steel. This is considered to be due to the increase of the strain induced precipitation of VC in deformed austenite, through the increase of the super saturation of VC with the increase in the carbon content. (2) The ferrite-pearlite structures of 0.4%C-0.3%V steels hot-deformed at non-recrystallization temperature (below 1223K) are refined remarkably, through the increase of the ferrite nucleation site consisted of the flattend austenite grain boundary and the annealing twin formed in the austenite grain. (3) 0.4%C-0.3%V steels hot-rolled at non-recrystallization temperature on the practical mill have superior toughness in spite of high tensile strength over 900N/mm^2 because of the microstructure refinement through the non-recrystallization austenite deformation.
- 社団法人日本鉄鋼協会の論文
- 1996-11-01
著者
関連論文
- 中炭素非調質鋼の疲労強度に及ぼすミクロ組織の影響
- ベイナイト非調質鋼の疲労強度特性
- 機械構造用非調質鋼の疲労強度に及ぼす加工熱処理の影響
- 455 非調質鋼の疲労強度におよぼす熱間鍛造条件の影響(棒鋼, 線材, 材料, 日本鉄鋼協会第 113 回(春季)講演大会)
- 658 高靱性フェライト・ベイナイト型非調質鋼(被削性・切削・条鋼・線材, 材料, 日本鉄鋼協会第 111 回(春季)講演大会)
- 自動車用特殊鋼の機能
- 116 地疵の生成におよぼす不活性雰囲気造塊の影響(非金属介在物, 日本鉄鋼協会第 68 回(秋季)講演大会講演論文集 (I))
- 浸炭処理される駆動系鍛造部品の動向と課題
- 中炭素非調質鋼のミクロ組織に及ぼすバナジウムと加工熱処理の影響
- 自動車用熱間鍛造非調質鋼における組織制御技術