超深絞り用 Ti 添加極低炭素鋼の製造
スポンサーリンク
概要
- 論文の詳細を見る
Ti-stabilized extra-low carbon steel sheet has excellent deep drawability. A series of investigations on vacuum decarburization, deoxidation and Ti addition has been carried out. The followings have been found through these trials, and Ti-stabilized steel (≤0.006%C) has been successfully manufactured.(1) In order to obtain extra-low carbon content, it is necessary that the DH vessel bottom should have a large area and a shallow steel bath.(2) To obtain suitable Ti content, complete Al deoxidation is necessary before Ti addition.(3) Too long DH treatment after alloy additions is ineffective to eliminate oxide inclusion.(4) Much amount of oxide inclusion is located near the skin of an ingot, and can be cut off by hot scarfing after slabbing.(5) Petrolic mold coating material or a cast iron stool causes an increase in carbon content of ingots.
- 1973-02-01
著者
関連論文
- 連続焼鈍による超深絞り用冷延鋼板の製造
- 200 Ti 添加鋼の r 値におよぼす製造要因の効果について(冷延鋼板, 加工・性質, 日本鉄鋼協会 第 85 回(春季)講演大会)
- 191 連続焼鈍による超深絞り用冷延鋼板の製造(冷延鋼板, 加工・性質, 日本鉄鋼協会 第 85 回(春季)講演大会)
- 超深絞り用 Ti 添加極低炭素鋼の製造
- 日本における圧延技術の進歩 (ストリップ表面処理特集)
- 圧延加工の現状と将来 (金属加工の将来展望)
- 食, 飲用罐工業と材料の変遷