實驗結果から得た焼結機構に關する一考察
スポンサーリンク
概要
- 論文の詳細を見る
After Sintering experiments using the Greenawalt sintering pan, we can obtain some conclusions about sintering practice, that is ; (1) It is possible to regulate the sintering conditions such as moisture of raw materials, mixing ratio, sintering time etc, by examinig the microstructure of sinter in the proceed of production. (2) Decreasing the lower limit of the size of sinter from 15 mm to 10 mm, we can expect the increase of yield of sinter by 13.6%, and the strength by 10.5%. But in this case, not the latter but the former contains bedding materials in it. (3) Comparing the shatter strength of each size of sinter (5∿10mm, 11-15mm, 16∿50mm over 50mm), we can find that the smaller the size of sinter the more the percentage of sinter keeping its own size before shatter test becomes.
- 社団法人日本鉄鋼協会の論文
- 1949-10-25
著者
-
浮田 清代志
日本鋼管京浜製鉄所
-
奥村 昌洋
日本鋼管川崎製鐵所
-
山田 千春
日本鋼管会社川崎製鉄所
-
山田 千春
日本鋼管川崎製鐵所
-
高野 廣
日本鋼管川崎製鐵所
-
浮田 清代志
日本鋼管川崎製鐵所
-
高野 廣
日本鋼管(株)
関連論文
- 170 管用丸鋼片の〓粉探傷機(耐熱鋼・ステンレス鋼・探傷法・その他, 加工・性質・分析・計測, 日本鉄鋼協会第 80 回(秋季)講演大会講演)
- 荷役機械保守の実例について
- (10)圧延機(潤滑油および潤滑特集)
- [108]金属圧延ロール用合成樹脂軸受の最近の発達(2.工業材料及び材料学)
- [300] 厚板及び中板の圧延に就て(18. 鋳造、鍛造及び熔接)
- [299] 刄物用硬質合金切削摩耗の過程(17. 工作機械及び工作法)
- [186]金属面の電気的方法に依る迅速なる研磨腐蝕方法(2.工業材料及び材料学)
- [185]耐蝕クロム鋼の表面硬化に就て(2.工業材料及び材料学)
- [32] 鋼の熔接性(18. 鋳造、鍛造及び熔接)
- [336] 100万V迄のX線の鋼に対する透過度(2. 工業材料及び材料学)
- 實驗結果から得た焼結機構に關する一考察
- 起重機の保守について
- 日本鉄鋼業の生産性 : 特に省力化技術について