焼入鋼旋削時のセラミック工具の初期欠損(第1報) : 初期欠損と切削条件
スポンサーリンク
概要
- 論文の詳細を見る
The early fracture is investigated experimentally that occurs in the turning of hardened steel with ceramic tools, and the occurrence condition is clarified. And a method of evaluation is propounded for the early fracture toughness. A turning test is carried out with hardened SUJ2 steel(HRC66) and ceramic tool. The critical cutting speed decided by one-minute criterion is found out, and the influences for the fracture of cutting conditions are clarified. The main findings are as follows : (1) Black ceramic tools show normal wear and long life at lower cutting speed. But they show suddenly early fracture at high speed. (2) The critical cutting speed becomes high according to the decreasing of feed rate, depth of cut and the increasing of corner radius. (3) The critical cutting speed is decided by the maximum undeformed chip thickness. (4) The early fracture is affected by rather the cutting temperature than the cutting force. (5) The early fracture toughness of various ceramics tools is evaluated by the maximum undeformed chip thickness and the critical cutting speed. (6) The early fracture is controlled by the coolant.
- 公益社団法人精密工学会の論文
- 1989-09-05
著者
関連論文
- 774 SUS 304 棒鋼の被削性 : ステンレス鋼の被削性 1(レール鋼, ロール材, 工具鋼, 軸受鋼, 摩耗, 切削性, 材料, 日本鉄鋼協会第 112 回(秋季)講演大会)
- 溝磨耗生成機構に関する基礎研究
- 焼入鋼の仕上げ切削(第1報) : 構成刃先の生成に及ぼす被削材硬さの影響
- 焼入鋼旋削時のセラミック工具の初期欠損(第2報) : 被削材硬さと切れ刃形状の影響
- FRM 振動切削時の工具摩耗
- 焼入鋼旋削時のセラミック工具の初期欠損(第1報) : 初期欠損と切削条件
- TiN薄膜による高速度鋼工具のクレ-タ摩耗抑制
- 切りくずの流出挙動観察のための一方法
- 旋削バイト寿命と加工物形状との関連について
- 旋削における切削温度測定の一方法