Wet plating such as chemical plating, electroplating is good technique. But its waste fluid are somewhat troublesome. The other hand it is said that the metallizing by dry plating has less adhesion. Therefore, latter method is employed. The speciemen are made from polyacetal (POM) and are molded by injection. POM's surface is directly metallized without precoating or pre-etching. Evaporated metals are Ni, Cu, Al and Cr, and ceramics TiN film is also tested. This investigation revealed adhesion between POM's surface and metal film or ceramic film. Obtained results are as follow. In the case of optically flat surface, they strongly adherered mutually, on the contrary, when the surface was extremly rough, then film peeled off easily. It seems to be indispensable that the cavity surfaces of the dies for injection molding are made carefully.
- 岡山理科大学の論文
- 1987-03-05
著者
関連論文
- Al-Si系およびAl-Ge系合金の時効処理による微細組織変化と疲労強度
- 微量Cu,Ge添加によるAl-1.2%Si合金の機械的性質改善(機械材料・材料加工II)
- Al-Mg-Si合金の疲労強度に及ぼす微量Fe,Cr添加の影響(機械材料・材料加工II)
- 448Kで時効した6000系アルミニウム合金の機械的性質
- Al-1.2%Si合金の機械的性質に及ぼすCu添加の影響
- Al-1.2%Si合金の時効に及ぼすGe添加の影響
- Al-4%Ge合金の疲労強度に及ぼす熱処理条件の影響
- 29p-P-6 非晶質GeSeのEXAFS
- 31p GK-7 固溶体Al-Cu合金に対する銅のK吸収端付近のEXAFSの測定
- Al-Zn-(Mg_2Si)合金中のG.P.zoneと焼入空孔の相互作用 : 格子欠陥
- Al-4%Ge 合金の時効組織と疲労強度
- Al-Zn 系合金の疲労特性に及ぼす表面処理の影響
- Al蒸着したAl-Zn合金の疲労強度
- Al-Zn合金の時効硬化と疲労強度に及ぼす微量Si添加の影響
- Al-Mg-Si系合金のセレーションに及ぼす時効処理の影響
- Al-Ge系合金の機械的性質に及ぼす熱処理の影響
- Al-Mg-Si系合金T6材の疲労強度
- Al-Zn系合金の機械的性質に及ぼす微量Cu添加の影響
- Al-Zn 系合金の機械的性質に及ぼす微量 Fe 添加の影響
- Al-2%Ge合金の引張特性に及ぼす時効の影響
- Al1.2%Si合金の時効処理による粒界近傍の組織変化と疲労強度
- Al-1.2%Si合金の疲労強度に及ぼす熱処理の影響
- 高濃度のZnを含有するAl-Zn合金の時効硬化と疲労強度
- 時効硬化したAl-Zn合金の疲労強度に及ぼす試料厚さの影響
- ポリアセタール表面への金属の真空蒸着
- アルミナセラミックス用結合剤及び滑剤の開発 : PVA及びステアリン酸系について
- 集合組織を有する金属材料の降伏曲面に関する研究
- Al-3mass%Mg合金の疲労強度に及ぼす表面層の影響
- 低濃度Al-Zn合金中のクラスターについて
- Al-Zn-Mg_2Si,Al-Zn-Mg_2GeおよびAl-Ag-Mg_2Si合金の初期時効