Initial dissolution rate of a Japanese simulated high-level waste glass P0798 as a function of pH and temperature measured by using micro-channel flow-through test method
スポンサーリンク
概要
- 論文の詳細を見る
- 2012-04-01
著者
-
Inagaki Yaohiro
Department Of Applied Quantum Physics & Nuclear Engineering Kyushu University
-
IDEMITSU Kazuya
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University
-
ARIMA Tatsumi
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University
-
Tatsumi Arima
Department Of Applied Quantum Physics & Nuclear Engineering Kyushu University
-
Idemitsu Kazuya
Department Of Applied Quantum Physics & Nuclear Engineering Kyushu University
-
MAKIGAKI Hikaru
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University
-
MITSUI Sei-Ichiro
Geological Isolation Research and Development Directorate, Japan Atomic Energy Agency
-
NOSHITA Kenji
Hitachi Research Laboratory, Hitachi Ltd.
-
Makigaki Hikaru
Department Of Applied Quantum Physics & Nuclear Engineering Kyushu University
-
Mitsui Sei-ichiro
Geological Isolation Research And Development Directorate Japan Atomic Energy Agency
-
IDEMITSU Kazuya
Department of Applied Quantum Physics & Nuclear Engineering, Kyushu University
関連論文
- Aqueous Corrosion Behavior of Glass Phase of Simulated Low Level Waste Form Produced by In-can Type Induction-Heated Melting
- Aqueous Dissolution of Silver Iodide and Associated Iodine Release under Reducing Conditions with FeCl_2 Solution
- Concentrations of Radiocarbon and Isotope Compositions of Stable Carbon in Food
- Behavior of Fission Products Zirconium and Barium in Fast Reactor Fuel Irradiated to High Burnup
- Research of Zirconia-based Oxide Spheres for Cermet Fuel: Production through Internal Gelation Process and the Compatibility with Zr, Zircaloy-4 and Si
- Corrosion Products from Carbon Steel Formed in Compacted Bentonite under Reducing Conditions
- Burning of MOX fuels in LWRs ; fuel history effects on thermal properties of hull and end piece wastes and the repository performance
- Initial dissolution rate of a Japanese simulated high-level waste glass P0798 as a function of pH and temperature measured by using micro-channel flow-through test method
- Corrosion Behavior of a Powdered Simulated Nuclear Waste Glass in the Presence of Bentonite.
- Volumetric change of simulated radioactive waste glass irradiated by electron accelerator.