Effect of Repeated Tempering on Hardness and Retained Austenite of High Chromium Cast Iron Containing Molybdenum
スポンサーリンク
概要
- 論文の詳細を見る
- Japan Institute of Metalsの論文
- 2010-07-01
著者
-
MATSUBARA Yasuhiro
Kurume Technical College
-
SASAGURI Nobuya
Kurume National College of Technology
-
Sasaguri Nobuya
Kurume National Coll. Of Technol.
-
INTHIDECH Sudsakorn
Faculty of Engineering, Mahasarakham University
-
BOONMAK Khatawut
Faculty of Engineering, Mahasarakham University
-
SRICHAROENCHAI Prasonk
Faculty of Engineering, Chulalongkorn University
-
Inthidech Sudsakorn
Faculty Of Engineering Mahasarakham University
-
Inthidech Sudsakorn
Faculty Of Engineering Mahasarakam University
-
Matsubara Yasuhiro
Kurume National College Of Technology
-
Sricharoenchai Prasonk
Department Of Metallurgical Engineering Faculty Of Engineering Chulalongkorn University
-
Boonmak Khatawut
Faculty Of Engineering Mahasarakham University
関連論文
- Quantitative Evaluation of Solidification Brittleness of Weld Metal during Solidification by In-Situ Observation and Measurement (Report II) : Solidification Ductility Curves for Steels with the MISO Technique(Materials, Metallurgy & Weldability)
- Solidification of High Chromium Cast Iron Substituted by 25 to 70mass%Ni for Fe
- Analysis of Carbides in Multi-component White Cast Iron for Hot Rolling Mill Rolls
- Effect of Substrate Temperature, Biasing and Sputter Cleaning on the Structure and Properties of Nanostructured TiB_2 Coatings on High Speed Steel
- Improvement in Adhesion of Sputtered TiB_2 Nano-Compostite Coatings onto High Speed Steel by a Chromium Interlayer
- Effect of Repeated Tempering on Hardness and Retained Austenite of High Chromium Cast Iron Containing Molybdenum
- Effect of Alloying Elements on Heat Treatment Behavior of Hypoeutectic High Chromium Cast Iron
- Effects of Chemical Composition and Heat-Treatment on Abrasion Wear Behavior of High Alloyed White Cast Iron
- Hot Ductility of High Purity Steels Containing Niobium
- Effect of Alloying Elements on Variation of Micro-Hardness during Heat Treatment of Hypoeutectic High Chromium Cast Iron
- Two-Body and Three-Body Types Abrasive Wear Behavior of Hypoeutectic 26 mass% Cr Cast Irons with Molybdenum