Development of a self-etching primer with higher shelf life and greater dentin bond stability
スポンサーリンク
概要
- 論文の詳細を見る
To examine the effects from the chemical structure of acidic methacrylate monomers on the primer’s shelf life, N-methacryloyl-2aminoethylphosphonic acid (NMEP)- N-methacryloyl glycine (NMGly), 2-methacryloyloxyethyl dihydrogen phosphate (MEP)-NMGly and 10-methacryloyloxydecyl dihydrogen phosphate (MDP)-NMGly primers were designed. Immediately after preparation, these primers were stored at 40°C for 0, 6 and 14 weeks. At the end of each storage period, 13C NMR observations were performed. Shear bond strengths of resin to dentin, conditioned by non-stored or stored primers, were measured. Alteration rates of these primers were strongly dependent on the chemical structure of acidic methacrylate monomers. The NMEP-NMGly primer exhibited noticeably higher hydrolytic stability and greater bond strength stability than MEP-NMGly and MDP-NMGly primers. These results demonstrated that methacryl amide monomers, NMEP and NMGly, are more advantageous than methacryl ester monomers. To develop self-etching primers with longer shelf life, it is essential to utilize acidic and hydrophilic methacryl amide monomers.
- 2010-01-01
著者
-
MA Shen
Department of Dental Materials, Nihon University School of Dentistry at Matsudo
-
Ma Shen
Department Of Dental Biomaterials Nihon University Graduate School Of Dentistry At Matsudo
関連論文
- Effect of Solvent Type on the Degradation of 4-MET
- Development of a self-etching primer with higher shelf life and greater dentin bond stability