The effective thermal conductivity of a Li4SiO4 pebble bed was measured by the hot wire method. The bare and silica-coated Nichrome heaters were used as the hot wires. At 975 K, effective thermal conductivity was not measured correctly by the bare hot wire. This is due to the fact that the electrical signal of a bare thermocouple is distorted due to the electrical conductivity of Li4SiO4. Using a silica-coated hot wire, effective thermal conductivity can be measured at temperatures ranging from room temperature to 975 K. The effect of the coating layer on the measured effective thermal conductivity was estimated to be small and corresponded to the experimental data. The hot wire method with silica coating can be applied to other ceramic breeder materials.
- 2009-06-01
著者
-
AKIBA Masato
Japan Atomic Energy Research Institute
-
Akiba Masato
Japan Atomic Energy Agency
-
TANIGAWA Hisashi
Japan Atomic Energy Agency
-
TANAKA Yuichiro
Interdisciplinary Graduate School of Engineering Sciences, Kyushu University
-
ENOEDA Mikio
Japan Atomic Energy Agency
-
Enoeda Mikio
Japan Atomic Energy Agency Fusion Res. And Dev. Directorate
-
Tanaka Yuichiro
Interdisciplinary Graduate School Of Engineering Sciences Kyushu University
関連論文
- Deuterium Retention in Tungsten Mixed Carbon Dust
- Morphology and Hydrogen Retention of Carbon Dust Produced by Hydrogen Discharges in JT-60 (第44回真空に関する連合講演会プロシーディングス--2003年11月12日〜14日,東京)
- Assessment of Applicability of Two-Fluid Model Code ACE-3D to Heat Transfer Test of Supercritical Water Flowing in an Annular Channel
- Thermal Conductivity Measurement with Silica-Coated Hot Wire for Li_4SiO_4 Pebble Bed
- Development of Supercritical Pressure Water Cooled Solid Breeder Blanket in JAERI
- Removal of Deuterium in Lithium Titanate by Sweep Gas Exposure