Fast Nanoimprint Thermal Lithography Using a Heated High-Aspect Ratio Mold
スポンサーリンク
概要
- 論文の詳細を見る
The throughput of the thermal nanoimprint lithography is improved. The proposed process uses a high-aspect ratio mold. The mold is heated to temperatures above the glass transition temperature of the resist, and only the top part of the mold is used to press the resist. The mold press time, the resist cooling time, and the mold releasing time can be reduced. A line pattern having a width of 100 nm and a pitch of 400 nm, and a dot pattern having a diameter of 75 nm and a pitch of 200 nm were successfully transferred to the resist using SiC molds. The imprint time was 5 s.
- 2006-12-25
著者
-
Nakada Yoshinobu
Institute Of Symbiotic Science And Technology Tokyo University Of Agriculture And Technology
-
Ninomiya Kenrou
Institute of Symbiotic Science and Technology, Tokyo University of Agriculture and Technology, 2-24-
-
Takaki Yasuhiro
Institute of Symbiotic Science and Technology, Tokyo University of Agriculture and Technology, 2-24-
-
Takaki Yasuhiro
Institute Of Symbiotic Science And Technology Tokyo University Of Agriculture And Technology
-
Ninomiya Kenrou
Institute Of Symbiotic Science And Technology Tokyo University Of Agriculture And Technology
関連論文
- Fast Nanoimprint Thermal Lithography Using a Heated High-Aspect Ratio Mold
- Three-Dimensional Print Using a One-Dimensional Screen Technique
- Increase in Depth of Field of Eyes Using Reduced-View Super Multi-View Displays