Wear of MgO-C Bricks Lining a RH Lower Vessel
スポンサーリンク
概要
- 論文の詳細を見る
- 2004-09-01
著者
-
Koyake Tamiatsu
Shinagawa Refractories Co. Ltd.
-
Suto Minoru
Shinagawa Refractories Co. Ltd.
-
KAWATA YOUSUIKE
Shinagawa Refractories Co., Ltd.
-
Kawata Yousuike
Shinagawa Refractories Co. Ltd.
関連論文
- Effect of Thermal Cycling on the Corrosion Resistance of MgO-C Bricks (2^ Report)
- Low Permeability Chrome-free Bricks for Secondary Refining Furnaces
- Low Permeability Magnesia-Chrome Bricks for AOD and VOD Vessels
- Iron-Oxide Corrosion of Magnesia-Chrome Bricks in the RH-OTB Degasser
- Dynamic Properties of Basic Bricks for Secondary Refining Furnaces, Evaluated by Torsion Testing
- Development of Low Carbon MgO-C Bricks with High Spalling Resistance
- Wear of MgO-C Bricks Lining a RH Lower Vessel
- Improvement on Fracture Toughness of MgO-C Bricks
- Improvement of Slag Infiltration Resistance of Unburned Al_2O_3-MgO Bricks