An Evaluation on Helium-Embrittlement-Resistance of Low Activation Ferritic/Martensitic Steel F82H
スポンサーリンク
概要
- 論文の詳細を見る
- 一般社団法人 日本原子力学会の論文
- 1999-08-25
著者
-
NAGAKAWA Johsei
National Institute for Materials Science
-
YAMAMOTO Norikazu
National Institute for Materials Science
-
Shiba Kiyoyuki
Tokai Research Establishment Japan Atomic Energy Research Institute
-
Nagakawa Johsei
National Institute For Materials Science (nims)
-
Yamamoto Norikazu
National Institute For Materials Science (nims)
関連論文
- Fatigue Properties of Helium Injected F82H-IEA Heat Material
- Fatigue Behavior of Cold-Worked 304 Stainless Steels under In-Situ Irradiation at 300℃
- Irradiation-Induced Deformation in Cold-Worked SUS 304 Stainless Steel
- Creep Behavior of 8Cr2WVTa Martensitic Steel Designed for Fusion DEMO Reactor : An Assessment on Helium Embrittlement Resistance(Special Issue on Creep and Fatigue at Elevated Temperatures)
- SB-01-1(020) Creep Behavior of 8Cr2WVTa Martensitic Steel Designed for Fusion DEMO Reactor : An Assessment on Helium Embrittlement Resistance(Materials Performance in Nuclear Application 1)
- An Evaluation on Helium-Embrittlement-Resistance of Low Activation Ferritic/Martensitic Steel F82H
- Void Swelling of Proton Irradiated Fe-15Cr-20Ni Ternary Alloy
- Effects of Implanted Deuterium on In-Situ Irradiation Fatigue Behaviors of Cold-Worked 316 Stainless Steel at 60 and 300℃
- In-Beam Stress Corrosion Tests for Welded 308 Stainless Steel in Pure Water at 473 K