Nanocrystallization Characteristics of Amorphous (Fe0.99Mo0.01)78B13Si9 and Fe78B13Si9 Alloys Treated by Shock Wave
スポンサーリンク
概要
- 論文の詳細を見る
It is found that these amorphous alloys have been transformed into crystalline phase with grain size of 20–40 nm after annealing at temperature from 450–550$^\circ$C for 30 min. Some new phases such as Fe3Si are observed and the lattice constant of $\alpha$-Fe is shortened. These can not be explained by the previous theory about process of diffusion, nucleation and growth of the crystals.Instead, we explain the experimental results by the model of free volume and shearing deposition. If properly applied, shock wave treatment of amorphous alloys would be a promising method for synthesizing new crystalline phases of multi-component systems.
- INSTITUTE OF PURE AND APPLIED PHYSICSの論文
- 2001-03-15
著者
-
Liu Ying
National Laboratory Of Antennas And Microwave Technology Of Xidian University
-
Liu Zuo
Department Of Physics Yunnan Normal University
-
Wang Guang
National Laboratory of Solid State Microstructures and Department of Physics, Nanjing University
-
Liu Zuo
Department of Physics, Yunnan University, Kunming 650091, P. R. China
関連論文
- Effects of Deletion and Shift of the A20-B19 Disulfide Bond on the Structure, Activity, and Refolding of Proinsulin
- Flexibility Exists in the Region of [A6-A11, A7-B7] Disulfide Bonds during Insulin Precursor Folding
- Nanocrystallization Characteristics of Amorphous (Fe_Mo_)_B_Si_9 and Fe_B_Si_9 Alloys Treated by Shock Wave
- Realization of Gain Improvement Using Helix-Monopole Antenna for Two-Way Portable Radio(Antennas and Propagation)
- Nanocrystallization Characteristics of Amorphous (Fe0.99Mo0.01)78B13Si9 and Fe78B13Si9 Alloys Treated by Shock Wave
- Flexibility Exists in the Region of [A6-A11, A7-B7] Disulfide Bonds during Insulin Precursor Folding