概要
- 論文の詳細を見る
Surface temperature near the end part of the molten pool in TIG arc welding for 2.3 mm thick mild steel plates was measured with a Silicon monochromatic optical pyrometer. Relationships between the surface temperature and the reverse side bead width were investigated under various conditions.<BR>Results of this experiment are summarized as follows.<BR>(1) The effect of TIG arc on the temperature measurement disappeared at the position about 10 mm away from the center of the arc.<BR>(2) It was concluded from the results of measurements that the mutual relation existed between the surface temperature near the rear end part of the molten pool and the reverse side bead width.
- 一般社団法人 溶接学会の論文
一般社団法人 溶接学会 | 論文
- Special issue. New frontiers of welding technology. Design of super sky scyaper and its conection and welding.
- The Microstructure of Iron Base Binary Weld Metals (Report 2):Effect of ferrite formers
- The Microstructure of Iron Base Binary Weld Metals (Report 1):Effect of austenite forming type alloying elements
- The Behavior of Hydrogen in Arc Welding (Report 4):Hydrogen dissolution into submerged arc weld metal
- A Study on Submerged Arc Welding of HT-80 Steel (Report 1):Cracking and Hydrogen in submerged arc weld metal