The formation of the Cd-bearing ferrite by the air oxidation of an aqueous suspension.
スポンサーリンク
概要
- 論文の詳細を見る
When the Cd<SUP>2+</SUP>/Fe<SUB>total</SUB> ratio in the initial solution is below 0.1, almost all cadmium ions are incorporated into the ferrite with the spinel-type structure by the air oxidation of an aqueous suspension at a pH 9.0 and at 65 °C. The Cd-bearing ferrite thus obtained is a ferromagnet and is oxidized to form a completely oxidized Cd-bearing ferrite at 150 °C in the air; this ferrite is still a ferromagnet and belongs to the Fe<SUB>2</SUB>O<SUB>3</SUB>–CdFe<SUB>2</SUB>O<SUB>4</SUB> binary system, with the same spinel type structure. When the Cd<SUP>2+</SUP>/Fe<SUB>total</SUB> ratio in the initial solution increases to 0.5, the crystalline phases formed is complicatedly changed; the products are also significantly affected by the pH value of the suspension. The most favorable pH value at 65 °C to form the Cd-bearing ferrite is proposed to be 10.0.
- 公益社団法人 日本化学会の論文
著者
-
Tamaura Yutaka
Department Of Chemistry Tokyo Institute Of Technology
-
KATSURA Takashi
Department of Chemistry
-
KANZAKI Tadao
Department of Chemistry, Tokyo Institute of Technology
-
Kanzaki Tadao
Department Of Chemistry Tokyo Institute Of Technology
-
Takei Katsumori
Department of Chemistry, Tokyo Institute of Technology
-
Kaneko Ken
Department of Chemistry, Tokyo Institute of Technology
関連論文
- Preparation of Co_xFe_O_4 Films in Aqueous Solution at 120-200℃ by "Hydrothermal Ferrite Plating"
- Magnetic and Mossbauer Studies of a New Compound YFe_2O_4
- PRECONCENTRATION OF TRACE AMOUNT OF CADMIUM IN WATER BY "FERRITE PROCESS"
- Maskless Patterning of Ferrite Film by Selected Area Film Growth in Aqueous Solution by "Laser-Enhanced Ferrite Plating"
- High-Rate Deposition of Ferrite Films in Aqueous Solution by Light-Enhanced Ferrite Plating
- Ferrite Plating of (Fe, Ni, Zn) _3O_4 Films in Aqueous Solution by an "Improved" Spray-Spin-Coating Method : Chemistry (incl. physical process)
- Ferrite-Plating in Aqueous Solution : A New Method for Preparing Magnetic Thin Film
- Phase equilibria in the Ln2O3-V2O3-V2O5 (Ln=Eu and Yb) systems at 1200.DEG.C.
- Phase equilibria in the La2O3-V2O3-V2O5 system at 1200.DEG.C.
- The formation of the Cd-bearing ferrite by the air oxidation of an aqueous suspension.
- Aluminium-bearing ferrite formation from .GAMMA.-FeOOH in an aqueous suspension.
- Formation of Zn-bearing ferrite by air oxidation of aqueous suspension.
- Role of the intermediate layer and factors determining chemical composition of the film in the electroless ferrite-plating.
- The transformation of .GAMMA.-FeO(OH) to Fe3O4 and green rust II in an aqueous solution.
- Thermochemical Properties of Lanthanoid-Iron-Perovskite at High Temperatures
- Phase Equilibria in the V2O3–VO2 System at High Temperatures
- The Phase Equilibria in the FeO-Fe2O3-V2O3 System at 1500°K
- Phase equilibria in the Gd2O3-V2O3-V2O5system at 1200.DEG.C.
- Phase equilibria in the Ln2O3-V2O3-V2O5 (Ln=Pr,Tb, and Y) systems at 1200.DEG.C.
- Phase equilibria in Sm2O3-V2O3-V2O5 system at 1200.DEG.C.
- The formation of Mg-bearing ferrite by the air oxidation of aqueous suspensions.
- The Activity of Dilute Sodium in Liquid Au-Na Alloy
- The Thermodynamic Properties of the Nonstoichiometric Ceric Oxide at Temperatures from 900 to 1300°C
- The Standard Free Energy of the Formation of LaFeO3 at 1204°C