The interdiffusion coefficients of the Fe-Ni system were determined in hydrogen atmosphere over the temperature range from 1000°to 1350°C on four couples with different combinations of plate and powder compact. The concentration gradients were measured with an electron probe microanalyser, and the diffusion coefficients were calculated by the Matano analysis. The results showed that the activation energy for the interdiffusion in the couple of Fe/Ni plate varies from 60 to 70 Kcal/mol with the decreasing nickel contents, while it is about 50 Kcal/mol in the couple of Fe/Ni powder compact. This suggests that the diffusibility of both elements are enhanced in the powder side zone of the couple. The enhanced diffusibility is also observed on both couples of Fe plate/Ni powder compact and Fe powder compact/Ni plate.<BR>The Kirkendall marker movement in a couple of powder compact indicates that iron atoms diffuse more rapidly than nickel atoms, and the ratio of the intrinsic diffusion coefficient of iron and nickel is about 2 at 1300°C. Furthermore, there exist a highly porous zone on the iron side and a highly densified zone on the nickel side across the initial interface.
- 社団法人 粉体粉末冶金協会の論文
著者
関連論文
- 準安定オーステナイト系ステンレス鋼における加工誘起マルテンサイトの拡散型逆変態に及ぼす前加工の影響
- 準安定オーステナイト系ステンレス鋼におけるせん断型逆変態オーステナイトの細粒化機構に及ぼす前加工の影響
- Mo を含む準安定オーステナイト系ステンレス鋼の逆変態機構と機械的性質
- 準安定オーステナイト系ステンレス鋼のα'→γ逆変態に及ぼす炭素の影響
- 準安定オーステナイト系ステンレス鋼における加工誘起マルテンサイトの逆変態機構
- 加工誘起マルテンサイトの逆変態による結晶粒超微細化に適したFe-Cr-Ni合金成分の検討
- 準安定16-10ステンレス鋼の結晶粒超微細化による強化
- 800 Mo を含むオーステナイト系ステンレス鋼のα'→γ逆変態による結晶粒超微細化(微細粒, 超塑性, 萌芽・境界技術, 日本鉄鋼協会第 114 回(秋季)講演大会)
- 540 準安定オーステナイト系ステンレス鋼における加工誘起マルテンサイトの逆変態機構(ステンレス鋼, 極低温用鋼, 材料, 日本鉄鋼協会第 113 回(春季)講演大会)
- 504 超微細粒オーステナイト系ステンレス鋼の変態挙動と機械的性質(ステンレス鋼 (I), 材料, 日本鉄鋼協会第 111 回(春季)講演大会)