Recovery of Calcium from BF Slag and Synthesis of Zeolite A Using Its Residue
スポンサーリンク
概要
- 論文の詳細を見る
The elution and recovery of Ca from blast furnace slag and the alkali hydrothermal synthesis of zeolite A using the residue from the elution treatment were investigated using a ball-milling-type reaction vessel. The superior elution was obtained by using citric and formic acid solutions from which Ca could be selectively eluted from the slag. Whereas hydrochloric acid solution and ion-exchanged water were ineffective for Ca elution. Ca ions eluted in the solution were recovered as calcium formate by evaporation of water. From the formic acid eluted slag residue after three elution treatment cycles of the slag for 7.2 ks, zeolite A was synthesized in 1 mol/L NaOH solution with a reaction time of 86.3 ks at 343 K, without the addition of any other materials.
論文 | ランダム
- リンクパワーオフによるネットワーク省電力化のための高速トポロジ計算手法(グリーンICTとQoE,一般)
- B-12-5 MiDoRi GMPLSプロトコル拡張の提案(B-12.フォトニックネットワーク,一般セッション)
- R&Dホットコーナー ソリューション 光IP連携サーバのプラットフォーム技術
- B-12-32 PCE discoveryによる経路計算要求の輻輳制御に関する検討(B-12.フォトニックネットワーク,一般講演)
- IPオプティカルネットワークにおける光IP連携サーバによるマルチレイヤトラヒックエンジニアリング (特集 光IPネットワーキング技術の展望と最新動向)