In vitro evaluation of shear bond strength of veneering ceramics to zirconia
スポンサーリンク
概要
- 論文の詳細を見る
The bond strength between veneering ceramic and zirconia framework is the weakest link in the layered structure. To investigate the shear bond strength (SBS) of veneering ceramics to zirconia, four types of zirconia ceramics (Zirkonzahn, Cercon, Lava, DC-Zirkon) were selected. For each zirconia system, 30 disk specimens were layered with IPS e.max Ceram, Vita VM9, and a manufacturer-recommended veneering ceramic. SBS test was conducted, and fracture surface analysis was also performed to determine the failure modes. One-way ANOVA, two-way ANOVA, and Tukeys HSD tests were used to analyze the data. On shear bond strength between zirconia and their recommended veneering ceramics, statistically significant differences were observed among the different zirconia systems (p<0.001). DC-Zirkon exhibited the highest SBS value (40.49±8.43 MPa), followed by Lava (27.11±2.72 MPa), Zirkonzahn (24.46±3.72 MPa), and Cercon (20.19±5.12 MPa). On shear bond strength to IPS e.max Ceram and Vita VM9, significantly lower (p<0.001) were observed for these veneering ceramics than their recommended veneering ceramics for DC-Zirkon and Lava. For Zirkonzahn and Cercon, similar SBS values were observed for all kinds of veneering ceramics (p>0.05). In conclusion, the bonding of manufacturer-recommended veneering ceramic to the zirconia framework differed according to zirconia type.
論文 | ランダム
- 日本企業における国際的R&D活動成果の輩出構造に関する分析
- 中国日系企業の経営と課題
- 代地を通してみる名主支配に関する研究--「町鑑」を中心に
- 平成二二年度[関西大学]哲学会春季大会 研究発表要旨 鶴亭の作風とその分類--江戸時代における長崎派の一考察
- 江戸の古本屋(34)古本屋の起源(4)