Serial Batch Elution of Electric Arc Furnace Oxidizing Slag Discharged from Normal Steelmaking Process into Fresh Water
スポンサーリンク
概要
- 論文の詳細を見る
The serial batch leaching test of an electronic arc furnace oxidizing slag was performed on the basis of JIS K 0058-1 to investigate the safety of the slag and to clarify the elution mechanism. The slag which was discharged at the time of refining of normal steel was used for this experiment. The slag was dissolved in water whose initial pH was 6.0. After that, the slag was naturally dried. This operation was performed 12 times successively.The dissolution behaviors of Ca and Mg were expressed by the parabolic law. That of Si was expressed by the linear law. The dissolutions of them from the slag were controlled by the diffusion through pore and the surface layer through the surface layer where compositions of FeO and Al2O3 were high. Generally, the dissolve concentrations decreased with the increase in the number of the elution times. The environmentally regulated substances were not detected or less than the levels of the environmental quality standards for soil. Ba, Mn, Mo, K, Na, Sr and W were detected as minor element except for the environmentally regulated elements. Generally, the detected environmentally regulated substances and the other minor elements decreased with the number of the elution times. During the elution of the slag, the pH of the aqueous solution steeply increased initially, and it decreased afterwards. The pH decreased with the increase in the number of the elution times.
論文 | ランダム
- 硫化水素を含有する油井環境における金属の腐食
- 1079 跳躍動作の加速度特性(理学療法基礎系,一般演題(ポスター発表演題),第43回日本理学療法学術大会)
- 1263 歩行周期中に観測される生体時系列データの特性(理学療法基礎系45, 第42回日本理学療法学術大会)
- 705 立ち上がる動作の特徴(理学療法基礎系36, 第42回日本理学療法学術大会)
- 998 ゲーム機を用いた運動療法による口腔内環境変化 : モグラ叩きと速歩の比較(生活環境支援系理学療法3,一般演題ポスター発表,理学療法の可能性,第41回日本理学療法学術大会)