Oxidation kinetics of Low-Sn Zircaloy-4 at the Temperature Range from 773 to 1, 573 K
スポンサーリンク
概要
- 論文の詳細を見る
Isothermal oxidation tests in flowing steam were performed on low-Sn Zircaloy-4 cladding tubes over the wide temperature range from 773 to 1,573 K in order to obtain oxidation kinetics applicable to various loss-of-coolant accident conditions of LWRs. The oxidation generally obeys a parabolic rate law for the examined time range up to 3,600 s at temperatures from 1,273 to 1,573 K, and for a limited time range up to 900 s from 773 to 1,253 K. A cubic rate law is preferable for evaluating the longer-term oxidation at 1,253 K and below. The parabolic rate law constant and the cubic rate law constant for measured weight gain were evaluated at every examined temperature, and Arrhenius-type equations were determined in order to describe the temperature dependence of the rate constants. It was indicated that the change of the oxidation kinetics from the cubic to the parabolic rate and the discontinuities in the temperature dependence of the rate constants are caused by the monoclinic/tetragonal phase structure change of ZrO2.
- 社団法人 日本原子力学会の論文
- 2003-04-25
著者
-
NAGASE Fumihisa
Japan Atomic Energy Agency
-
Nagase F
Japan Atomic Energy Res. Inst. Ibaraki
-
Uetsuka Hiroshi
Surface Chemistry Laboratory Kanagawa Academy Of Science And Technology Ksp East 404
-
Uetsuka Hiroshi
Japan Atomic Energy Research Institute
-
Uetsuka Hiroshi
Institute Of Materials Science University Of Tsukuba
-
Uetsuka Hiroshi
Department Of Reactor Safety Research Japan Atomic Energy Research Institute
-
Otomo Takashi
Japan Atomic Energy Research Institute
関連論文
- Identification of Radial Position of Fission Gas Release in High-Burnup Fuel Pellets under RIA Conditions
- Optimized Ring Tensile Test Method and Hydrogen Effect on Mechanical Properties of Zircaloy Cladding in Hoop Direction
- Behavior of High Burn-up Fuel Cladding under LOCA Conditions
- Oxidation of Fuel Rod under Dry Storage Condition
- Effects of Fuel Oxidation and Dissolution on Volatile Fission Product Release under Severe Accident Conditions
- Releases of Cesium and Poorly Volatile Elements from UO_2 and MOX Fuels under Severe Accident Conditions
- Fracture Behavior of Irradiated Zircaloy-4 Cladding under Simulated LOCA Conditions
- Irradiated Fuel Behavior under Power Oscillation Conditions
- Behavior of YSZ based Rock-Like Oxide Fuels under Simulated RIA Conditions
- Decrease of Cesium Release from Irradiated UO_2 Fuel in Helium Atmosphere under Elevated Pressure of 1.0 MPa at Temperature up to 2,773K
- Enhancement of Cesium Release from Irradiated Fuel at Temperature above 2,800 K
- Influence of Pressure on Cesium Release from Irradiated Fuel at Temperatures up to 2,773K
- Behavior of Coated Fuel Particle of High-Temperature Gas-Cooled Reactor under Reactivity-Initiated Accident Conditions
- Noncontact-Mode Atomic Force Microscopy Observation of α-Al_2O_3(0001) Surface
- Scanning Tunneling Microscopy Study of Surface Reconstructions of Rutile TiO_2(111)
- Structure-sensitivity of the Dynamics of CO Oxidation on Pd (111), Pd (110) and Polycrystalline Pd Surfaces : Infraed Chemiluminescence Study of the Product CO_2
- Infrared Chemiluminescence Study of Excited CO_2 Produced by Molecular - Beam CO Oxidation on Pt(111)
- Behavior of 60 to 78MWd/kgU PWR Fuels under Reactivity-Initiated Accident Conditions
- Fission Gas Release Behavior of High Burnup UO_2 Fuel under Reactivity Initiated Accident Conditions
- Behavior of Pre-hydrided Zircaloy-4 Cladding under Simulated LOCA Conditions
- Investigation of Hydride Rim Effect on Failure of Zircaloy-4 Cladding with Tube Burst Test
- Influence of Hydride Re-orientation on BWR Cladding Rupture under Accidental Conditions
- Effect of Pre-Hydriding on Thermal Shock Resistance of Zircaloy-4 Cladding under Simulated Loss-of-Coolant Accident Conditions
- Effect of Cooling History on Cladding Ductility under LOCA Conditions
- Atomic Force Microscope Topography of Nickel-Affected MoS_2 Model Catalysts
- CO_2 Sensing Properties of La-loaded SnO_2 Thin Films Prepared by Sputtering
- Oxidation kinetics of Low-Sn Zircaloy-4 at the Temperature Range from 773 to 1, 573 K
- B_4C/Zircaloy Reaction at Temperatures from 1, 173 to 1, 953 K
- Influence of Precipitated Hydride on the Fracture Behavior of Zircaloy Fuel Cladding Tube
- Irradiated Fuel Behavior under Power Oscillation Conditions
- Oxidation kinetics of Low-Sn Zircaloy-4 at the Temperature Range from 773 to 1, 573 K
- Influence of Hydride Re-orientation on BWR Cladding Rupture under Accidental Conditions