Nanostructured ZnO particles present in skin-care cosmetics and UVB/UVA sunscreen products generate strong oxidizing species (free radicals) when illuminated with UV radiation that can damages human skin and the horny layer. Damage to DNA by ZnO and other pigmentary ingredients in sunscreen formulations under artificial and solar UV exposure has been examined by Agarose gel electrophoresis using pUC 18 DNA plasmids (2686 base-pairs). Initial photoinduced oxidative damage done to DNA plasmids have been probed by nicking assays under in vitro conditions for ZnO. The effects of nanosize ZnO and CeO2 particles, and the newly developed CaO-doped and SiO2-coated CeO2 pigment are compared when subjected to artificial (75-W Hg-lamp) and solar UV radiation. Supercoiled DNA plasmids undergo one nick to produce the relaxed form, followed by a second nick yielding the linear form of the plasmids. The DNA constituents deoxyadenosine-5’-monophosphate (dAMP), guanosine-5’-monophosphate (GMP) and cytidine-5’-monophosphate (CMP) have been examined to assess the photooxidative damage done to these nucleotides under photocatalytic conditions using the cosmetic/sunscreen ZnO pigment. Adsorption of the nucleotide through the phosphate on the positively charged ZnO surface, followed by attack of the ribose/phosphate backbone by photogenerated · OH (and/or · OOH) radicals on the ZnO surface lead to the degradation of the dAMP’s ribose moiety and subsequently to decomposition of the adenine base residue. About 90% mineralization of the ribose/phosphate backbone occurred as evidenced by formation of H2PO4- ions after only 30 min of UV irradiation. The nitrogen atoms of the adenine base were converted to NO3- and NH4+ ions. About 45% of the organic carbons constituting the dAMP ribose backbone was mineralized to CO2 within 8 h of UV irradiation occurring through formation of carboxylic acid intermediates (succinic, acetic and formic), with 85% of the remaining nucleobase ultimately mineralized after 48 h of UV irradiation. Similar occurrences were seen for the GMP and CMP nucleotides.
著者
-
Koike Takayoshi
Frontier Res. Center For Global Environment Sci. Meisei Univ.
-
Hidaka Hisao
Frontier Res. Center For Global Environment Sci. Meisei Univ.
-
Sato Tsugio
Institute For Chemical Reaction Science Tohoku University
-
KOBAYASHI Hiroyuki
Frontier Research Center for the Global Environment Science, Meisei University
-
SERPONE Nick
Dipartimento di Chimica Organica, Università di Pavia
-
Serpone Nick
Dipartimento Di Chimica Organica Universita Di Pavia
-
KOIKE Takayoshi
Frontier Research Center for the Global Environment Science, Meisei University
-
Hidaka Hisao
Frontier Research Center for the Global Environment Science, Meisei University
関連論文
- Sunlight Photo-Assisted TiO2-Based Pilot Plant Scale Remediation of (Simulated) Contaminated Aquatic Sites
- Preparation of H_2Ti_4O_9 with High Specific Surface Area
- Mechanochemical Synthesis of Fluorine-Doped SrTiO_3 and Its Photo-oxidation Properties
- Preparation of Visible Light-Activated Titania Photocatalyst by Mechanochemical Method
- Non-stoichiometrically activated sintering of Ca_Sr_TiO_3
- Photocatalytic Degradation of Surfactants. XX. Photooxidation of Sodium ButylnaPhthalenesulfonates
- Hydrothermal synthesis of brookite type TiO_2 photocatalysts using a water-soluble Ti-complex coordinated by ethylenediaminetetraacetic acid(Aqueous Solution Science for Ceramic Processing II)
- Phase-Compositional and Morphological Control of Titania Nanoparticles via Low Temperature Dissolution-Reprecipitation Process in Liquid Media
- Decomposition of Carbon Dioxide by the Dielectric Barrier Discharge (DBD) Plasma Using Ca_Sr_TiO_3 Barrier
- Low-Temperature Synthesis and Mechanical Properties of SiC Porous Granules from Activated Charcoal with a Na Flux
- Synthesis of environmentally friendly ceramic materials via solvothermal reactions
- Solvent Extraction of Some Tervalent Lanthanoids with 1-(4-Ethylphenyl)-3-hydroxy- and 1-(4-Ethylphenyl)-3-hydroxy-2-methyl-4-pyridones
- One-Step Preparation of Blue-Emitting (La,Ca)Si3(O,N)5:Ce3+ Phosphors for High-Color Rendering White Light-Emitting Diodes
- Synthesis of Y2O3:Eu phosphor with various particles morphologies by solvothermal reaction in methanol–water system
- Synthesis and UV-shielding Property of Plate-like Potassium Lithium Titanate Coated with Calcia-doped Ceria Nanoparticles
- DNA Damage Photoinduced by Cosmetic Pigments and Sunscreen Agents under Solar Exposure and Artificial UV Illumination
- 界面活性剤の光分解(19)TiO2/H2O界面における非イオン性ドデカノイルアミド界面活性剤の光酸化メカニズム
- Microwaves in advanced oxidation processes for environmental applications : A brief review
- pH Dependence on Photodecomposition of Bisphenol A at TiO_2/H_2O Intefaces
- Synthesis of bundle-like CeO2 nanofibers and their sub-microstructures
- Photoinduced Characteristics of Metal-oxide Cosmetic Pigments by Agarose Gel Electrophoresis of DNA Plasmids in vitro under UV-illumination
- A New Oxygen Storage Capacity Material of a Tin-doped Ceria-Zirconia-supported Palladium-Alumina Catalyst with High CO Oxidation Activity