Measurements of magnetization and electrical resistivity were carried out for polycrystallineMn_{2-x}Co_{x}Sb (x = 0.17, 0.2) in magnetic fields up to 16 T in 10-620 K temperature range, in order to the firstordermagnetic transition (FOMT) affected by magnetic fields. The Curie temperatures for x = 0.17 and 0.2are estimated to be 488 K and 476 K, respectively. The FOMT temperatures (T_{t}) from the ferrimagneticto antiferromagnetic phase are estimated to be 75 K for x = 0.17 and 145 K for x = 0.2, respectively. Byapplying magnetic fields, T_{t} decreases and the thermal hysteresis becomes large. The results obtainedindicate that kinetic arrest effect in Mn_{2-x}Co_{x}Sb arises when T_{t} is lower than about 40 K.
- 2012-12-30
著者
関連論文
- 強磁場X線回折実験によるMn_CO_Sbの磁場中結晶評価
- 24aPS-47 圧力下磁化測定によるMn_Co_xSbのカイネティックアレスト効果の研究(24aPS 領域3ポスターセッション,領域3(磁性,磁気共鳴))
- Mn_{2-x}Co_{x}Sb (x = 0.17, 0.2) の強磁場中磁気特性
- 18aPSA-15 Mn_2Sb_Ge_x(0.05⪯x⪯0.2)磁気特性(18aPSA 領域3ポスターセッション(量子スピン・フラストレーション・遍歴・f電子・酸化物・化合物磁性),領域3(磁性,磁気共鳴))
- 26aPS-36 Mn_Cu_xSbの磁気特性及び伝導特性(26aPS 領域3ポスターセッション,領域3(磁性,磁気共鳴))
- 26aPS-35 圧力下におけるMn_Co_xSbの磁気緩和(26aPS 領域3ポスターセッション,領域3(磁性,磁気共鳴))
- タイトル無し
- 修士課程を振り返って