S0305-1-3 固体酸化物形燃料電池の電解質ピンホールの影響と数値解析(SOFC構成材料の信頼性(1))
スポンサーリンク
概要
- 論文の詳細を見る
The effects of defect in electrolyte on SOFCs have been studied by computational fluid dynamics (CFD) analysis. For defects, pinholes having the size from 10 μm to 100 μm in diameter were introduced to the 15 μm-thick electrolyte. Both structures of electrolyte on anode (electrolyte/anode) and cathode on electrolyte having cell structure (cathode/electrolyte/anode) were analyzed. At 800℃, dry hydrogen gas and air were introduced to anode and space/cathode, respectively, and CFD analyses were carried out. In case of the former structure, combustion was shown to be occurred in the space apart from the electrolyte, and increased temperature was calculated. In case of the latter structure, combustion area was shown to move toward anode area, and part of the anode was possibly oxidized.
- 一般社団法人日本機械学会の論文
- 2009-09-12
著者
-
松崎 良雄
東京ガス(株)技術研究所
-
藤田 顕二郎
東京ガス(株)フロンティア研究所
-
中村 和郎
東京ガス(株)フロンティア研究所
-
堀内 賢治
東京ガス(株)
-
中村 和郎
東京ガス(株)
-
染川 貴亮
東京ガス(株)
-
伊東 卓也
東京ガス(株)
-
松崎 良雄
東京ガス(株)
-
藤田 顕二郎
東京ガス(株)
関連論文
- シンクロトロン光を用いた固体酸化物形燃料電池セルの残留応力測定
- 支持膜式SOFCにおけるアノード基板内拡散
- Na_xCoO_単結晶を用いたテンプレート粒成長法及び反応性テンプレート粒成長法により合成した高配向Na_xCoO_セラミック
- Ni/YSZサーメット燃料極の電極性能に及ぼす粉体粒径の影響
- S0305-1-3 固体酸化物形燃料電池の電解質ピンホールの影響と数値解析(SOFC構成材料の信頼性(1))
- 単結晶を利用したNa_xCoO_2配向セラミックスの熱電特性
- S0305-2-2 支持膜式SOFCアノードの繰返し再酸化による劣化・破壊挙動(SOFC構成材料の信頼性(2))
- 先端材料応用技術 ダイヤモンドLEDによる高効率室温紫外発光
- 中温筒状横縞形SOFCの開発 (特集 SOFCの開発状況)
- 技術解説 ダイヤモンドのホモエピタキシャル成長と紫外発光ダイオードへの応用
- 家庭用小形固体酸化物燃料電池の開発
- 東京ガス(株)技術開発部における燃料電池開発紹介
- ダイヤモンド深紫外LED(ナノテクに託す未来の光源)
- ダイヤモンド紫外線発光素子
- 東京ガスにおけるSOFCの開発状況 (特集 SOFCの開発状況)
- 24pYE-6 ダイヤモンドにおける電子正孔液滴形成ダイナミツクスの観測(24pYE 新物質・高密度励起現象,領域5(光物性分野))
- 中温作動筒状横縞形SOFCスタックの耐久性・信頼性評価に関する集学的取り組み
- 9・2・9 燃料電池(9・2 各種エンジン,9.エンジンシステム,機械工学年鑑)