As the third alloying constituents, 0.5 to 6% of Cu, Ag, Zn, Hg, Al, Ti, Sn, Pb, Sb, Te, Cr, Mn and Ni were added alone or duplicately to the binary alloys of Mg-Cd, which contains 1 to 10% of the latter element. The Rockwell-hardness value of these alloys in the cast, annealed, quenched and aged state as well as the corrodibility against the distilled, the ordinary and the salt water were measured. The results obtained may be summarised as follows : The third constituents which harden the binary alloys most remarkably, are found to be Cu, Ni, Ag and Al, Sn, Mn, Zn, Sb and Hg harden the alloy to a certain extent, while the hardening effect of Pb and Te is very small. The alloys in the cast state show generally the highest heardeness value ; the annealing or quenching make them softer. A remarkable aging effect is found in the alloy containing Al or Zn. The addition of Ni, Cu and Ag shows a marked injurious effect on the eorrodibility of the Mg-Cd alloys. Al, Pb, Te and Sb make also the alloy corrodible. Although Sn, Zn, Mn, Hg and Ti do not improve the corrodibility of the binary alloys remarkably, the existence of these metals is at least not very harmful.
- 社団法人日本鉄鋼協会の論文
- 1935-02-25
著者
関連論文
- 第 2 回世界冶金会議出席報告(第 2 回世界冶金会議)
- 金属材料の熱処理中に起る組織変化に就て
- マグネシウム, カドミウム系を基礎とする多元系輕合金の研究(第 2 報)
- アルミニウム青銅の共析變態の性質に就て(第 5 報) : 變態に伴ふ組織の變化
- アルミニウム-亞鉛系合金のX線的研究
- 6) アルミニウムー亞鉛系合金の X 線的研究 : 幻燈使用(日本鐵鋼協會第拾五囘講演大會)
- マグネシウム・カドミウム系を基礎とする多元系輕合金の研究
- 14) マグネシユウム-カドミウム系を基礎とする多元輕合金の研究(日本鐵鋼協會第拾參囘講演大會(滿洲冶金學會聯合))
- 緩徐な冷却速度を與へる二三の燒入液に就いて
- 緩徐な冷却速度を與へる二三の燒入液に就いて(日本鐵鋼協會第拾貳囘講演大會)
- 15) 緩徐な冷却速度を與へる二三の燒入液に就いて(日本鐵鋼協會第拾貳囘講演大會)
- 14) ハーネマン金屬研究所製マルテンサイト活動寫眞の紹介(日本鐵鋼協會第拾貳囘講演大會)