Mo金属の単結晶成長と応用(<特集>機能素子・部品と単結晶育成)
スポンサーリンク
概要
- 論文の詳細を見る
A molybdenum single crystal with a large-scale and optional shape was easily obtained by the secondary recrystallization method. There are two fundamental factors for producing single crystal. The one is the presence of dis- persed second phases such as CaO and MgO, the other is the presensed of strong primary texture with fine-grained structure. A certain amount of CaO and MgO is effective as inhibitors on the grain growth behavior of worked molybdenum : initially restraining the normal grain growth by precipitation of CaO or MgO at primary recrystal- lized grain boundaries and conversely permitting the abnormal grain growth by decomposing them to single element at higher temperatures. The effect of initial grain size on the secondary grain growth behavior is important. In the case where the initial grain size was smaller than 50urn, a uniform and fine-grained recrystallized structure was obtained after annealed at 1500℃, whilst an abnormal grain growth occurred after annealed at 2000℃.
- 日本結晶成長学会の論文
- 1990-11-15
著者
関連論文
- 403 Moをインサート材にしたタングステンと銅との摩擦圧接
- 302 タングステンと銅との摩擦圧接(Moインサートの場合)
- 205 W-La_2O_3 の高温変形特性
- 4a-W-8 X線用モノクロメーターとしてのタングステン単結晶の評価
- 30a-ZB-5 X線用モノクロメーターとしてのタングステン単結晶の評価 II
- 熱延タングステン板の二次再結晶粒成長に及ぼすドープ剤の影響
- Mo金属の単結晶成長と応用(機能素子・部品と単結晶育成)