311 引張残留応力低減溶接方法の最適施工条件の確認試験
スポンサーリンク
概要
- 論文の詳細を見る
To reduce tensile residual stress in a welded region, a new cooling method-which rapidly applies a water shower behind the welding-torch-was developed. In the case of applying this method to the welding of austenitic stainless-steel, the welding and cooling conditions are the parameters for reducing the residual stress efficiently. To optimize these conditions, first, the effects of the parameters on residual stress were determined by FEM. Second, the optimized conditions were determined by using the FEM results and a robust design technique. To confirm the accuracy of the optimized conditions, residual stresses under optimized or non-optimized conditions were experimentally measured. Under the non-optimized conditions, it was found that the residual stresses were tensile. On the other hand, under the optimized conditions, all residual stresses were compressive. These measurements results agree well with the FEM analytical ones; thus it can be concluded that the optimized conditions to reduce tensile residual are valid.
- 社団法人日本機械学会の論文
- 2003-09-19
著者
関連論文
- 溶接直後水急冷による残留応力制御溶接方法の最適施工条件の検証(技術OS2-5 RBM・残留応力,技術OS2 電力設備の健全性)
- 311 引張残留応力低減溶接方法の最適施工条件の確認試験
- 723 水急冷による引張残留応力低減溶接方法の施工条件の最適化
- 419 SUS316Lステンレス鋼の溶接残留応力に及ぼす溶接後表面急冷の影響(材料工学)
- 原子炉機器に対するウォータージェットピーニング技術の開発(技術OS2-5 RBM・残留応力,技術OS2 電力設備の健全性)
- 102 WJP 処理による SUS304 鋼の表面改質と高サイクル疲労特性改善
- 618 ウォータージェットピーニング処理による SUS304 の高サイクル疲労特性改善
- 中靱性材料からなる圧力配管の LBB の成立性と限界き裂長さ
- A-55 原子力プラントへの形状記憶合金の適用
- 620 反射噴流型ウォータージェットピーニングによる残留応力の低減
- 繰返し荷重を受ける切欠材の弾塑性挙動
- 223 塑性的に拡げたパイプの残留応力解析
- 230 非破壊的簡易残留応力測定法の研究(2)
- 348 差込継手の残留応力分布に及ぼす斜角構造の影響(OS10-3 照射劣化,溶接部評価,OS10 エネルギー機器の経年変化に関する健全性評価手法の開発とその適用(2))
- α鉄のき裂進展の分子動力学シミュレーションにおける格子方位の影響 : 主要すべり方向を面内に含む場合
- 分子動力学法を用いたα鉄の延性き裂進展シミュレーションにおける温度調節と負荷速度の影響
- 内部時間理論を用いた任意繰返し塑性問題の材料定数の決定法