Mechanical Properties of MMC Based on Ti Alloy(Composite 3)
スポンサーリンク
概要
- 論文の詳細を見る
The purpose of this study is to investigate static mechanical properties of Ti-alloy matrix composite fabricated by HIP treatment. Ti-6Al-4V alloy and W short fiber were used for matrix and reinforcement, respectively. This MMC has been processed two kinds of secondary working. Secondary works are rotary-swaging or shape-forging. Ti-6Al-4V alloy is known as one of representative Ti-alloys and W short fiber possesses excellent mechanical properties, such as high tensile strength, hardness number and high melting temperature. According to these experimental results, it is found that hardness and tensile strength of this material increases with the increase in volume fraction of W short fiber. Tensile strength of shape forging material is lower than rotary-swaging one. In addition, the highest value of tensile strength achieved among the metal matrix composites for this material is 1520MPa under the condition of W fiber volume fraction of V_f=9% (secondary working is rotary-swaging).
- 一般社団法人日本機械学会の論文
- 2001-10-20
著者
-
NISHIDA S.
Faculty of Dental Science, Kyushu University
-
Son Sunyoung
Graduate School Saga Univ.
-
HAYASHI K.
Satellite Venture Business Laboratory, Saga Univ.
-
HATTORI N.
Faculty of Science & Engineering, Saga Univ.
-
NAKANO K.
Takada Industry Co. Ltd.
-
Hattori N.
Faculty Of Science & Engineering Saga Univ.
関連論文
- Size and Orientation of Masticatory Muscles in Patients with Mandibular Laterognathism
- Mechanical Properties of MMC Based on Ti Alloy(Composite 3)
- Static Mechanical Properties of Stainless Steel Fiber Reinforced Aluminum Composites(Composite 3)
- 844 Optimum Deformation Value of Notched Specimen by Roller-working